External Tooth Conical Lock Washer Description

  1. Enhanced Locking and Corrosion-Proof Performance
    • Formed from 18-8 / 304 austenitic stainless steel and work-hardened to ≈ 220 HV, the conical body stores spring energy while the outward-facing teeth dig into both the fastener underside and joint material, generating prevailing torque that blocks rotation under continuous vibration, shock loading, or thermal cycling.
    • The combined cone angle (≈ 8 °) and tooth height (0.30 – 0.45 mm on M3–M12 sizes) maintain preload as the joint settles, acting as a self-tensioning element that compensates for creep or gasket relaxation.
    • Chromium-oxide passivation delivers permanent immunity to salt spray, food-grade detergents, mild acids, and outdoor moisture across a -200 °C → +400 °C temperature window, removing the red-rust risk found in plated carbon-steel equivalents.
    • Verified by transverse-vibration (Junker) testing to retain ≥ 90 % of initial clamp force after 1 000 cycles and by cyclic salt-fog to resist pitting for 720 h without visible corrosion.
  2. बहुमुखी, क्रॉस-इंडस्ट्री अनुप्रयोग स्पेक्ट्रम
    • इलेक्ट्रॉनिक्स & Instrumentation: Secures PCB standoffs, display bezels, and EMI shields where low profile, electrical grounding through tooth contact, and non-magnetic material are critical.
    • चिकित्सा, भोजन & Pharmaceutical Equipment: Stainless construction tolerates aggressive wash-downs and autoclave cycles on mixer guards, sensor brackets, and sanitary piping clamps.
    • परिवहन & Marine Hardware: Locks lighting brackets, body panels, and deck fittings subjected to road shock, hull vibration, humidity, and salt-laden air.
    • मशीनरी, नवीकरणीय-ऊर्जा & Robotics: Maintains clamp integrity on sensor mounts, guard plates, cable glands, and turbine covers during high-cycle duty and rapid axis reversals.
  3. तकनीशियन-अनुकूल, समय बचाने वाला संचालन
    • Conical design centers automatically under bolt or nut faces, eliminating orientation concerns and accelerating blind, overhead, or gloved assembly.
    • Spring action compensates for torque scatter, allowing installers to use the same torque values as a plain washer without complex re-calculation; the result is consistent preload with standard tools.
    • Overall thickness of 0.5 – 1.0 mm adds minimal stack height, enabling retrofit into existing designs without longer fasteners or clearance changes.
    • Supplied bulk, in resealable pouches, or tape-and-reel strands for seamless integration with maintenance kits, bench stations, and high-speed pick-and-place feeders; optional laser-etched size code (≥ M4) simplifies sorting.
  4. प्रमाणित गुणवत्ता & दीर्घकालिक स्थायित्व
    • 100 % optical inspection confirms tooth height ± 0.02 mm, cone angle ± 0.5 °, and concentricity ≤ 0.05 mm TIR; Cp/Cpk data archived for ISO 9001, IATF 16949, and AS 9100 compliance.
    • Stress-relief tempering eliminates residual forming stresses, preserving high spring modulus for sustained bite through countless tighten/loosen cycles without galling mating surfaces.
    • Electropolished variants achieve Ra ≤ 0.4 µm for hygienic or decorative finishes while maintaining locking performance; low-outgassing options meet vacuum and clean-room standards.
    • QR-coded packaging ties every washer lot to melt chemistry, passivation batch, and inspection record, ensuring full traceability for safety-critical aerospace, medical-device, and infrastructure projects.

अतिरिक्त जानकारी

कलई करना

मैदान

व्यास

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

उत्पादक

गुक्सियांग

सामग्री

स्टेनलेस स्टील

पैकेज का आकार (सेमी)

30*20*20

शिपिंग अवधि

EXW गुआंग्डोंग प्रांत

एसकेयू

1,000,000 टुकड़े

उत्पाद संबंधी