Таблица перевода: дюймы в миллиметры

Таблица перевода дюймов в миллиметры

A complete inches to millimeters (mm) conversion table and two-way calculator for the fastener industry, engineering drawings, and everyday metric conversions. Find the exact metric equivalent of fractional inch sizes from 1/64" to 15/16", decimal sizes from 0.01" to 100", or convert any value in either direction with our instant calculator.

25,4
mm in 1 Inch (Exact)
12,7
mm in 1/2 Inch
60
Fractional Sizes Listed (1/64"–15/16")
0.0394
Inches in 1 Millimeter

Inches ⇄ Millimeters Converter

Inches to mm / mm to Inches Converter
Enter a value in either unit — the result updates instantly
25.4 mm
1 in × 25.4 = 25.4 mm

Inches to Millimeters Conversion Tables

Fractional Inches to mm (1/64" to 15/16")

Every fractional inch size from 1/64" to 15/16" with its exact millimeter value and a practical rounded equivalent. Use this table for imperial fasteners, wrench sizes, and fractional drill bits.

Fraction (in)Decimal (in)mm (Exact)mm (Approx)

Decimal & Whole Inches to mm (0.01" to 100")

Decimal inch values from 0.01" up to 100" for wide-range measurements — ideal for machine travel, plate thickness, and long-stroke dimensions.

Inches (")Миллиметры (мм)

Миллиметры & Centimeters to Inches (Reverse Lookup)

Convert metric sizes back to inches for метрический крепеж, tubing, and 3D printing filament diameters.

МетрикаInches (")

How to Convert Inches to Millimeters

FORMULA
d(mm) = d(in) × 25.4
5 in = 5 × 25.4 = 127 mm • 20 in = 20 × 25.4 = 508 mm • 1 mm = 1 ÷ 25.4 = 0.03937 in

One inch is defined as exactly 25.4 millimeters. To convert inches to millimeters, multiply the inch value by 25.4. To convert back, divide the millimeter value by 25.4. For centimeter and micron conversions use the quick formulas below:

ConversionFormula
Inches to millimetersValue (inches) × 25.4
Inches to centimetersValue (inches) × 2.54
Inches to micronsValue (inches) × 25.4 × 1,000

Where Inch-to-Millimeter Conversion Matters

Крепежи & Hardware

Imperial bolts, винты, и орехи are specified in fractional inches — 1/4"-20, 3/8"-16, 5/16"-18 — while metric counterparts use millimeter diameters. This table converts between UNC/UNF sizes and their metric equivalents.

Engineering Drawings & CAD

Blueprints and CAD models often mix imperial and metric dimensions. Use exact millimeter values from the fractional table to avoid tolerance and fit errors in machined parts.

3D Printing

Filament diameters (1.75 mm, 2.85 mm), nozzle sizes, and layer heights are metric; slicing software and STL models from US sources may quote inches. Reverse lookup helps you set the correct values.

Деревообработка & DIY

Lumber thickness, drill bits, and hardware from different regions mix units. A quick inches-to-mm conversion keeps shelf pins, dowels, and fasteners compatible.

Best Practices for Inch to mm Conversion

Quick Reference Tips

  • Always multiply inches by 25.4 — never approximate with 25 unless precision does not matter.
  • For fractional fastener sizes, use the fractional table above; the exact mm value avoids rounding drift in tapped holes.
  • Round to 2 decimals for general work, 3–4 decimals for machining tolerances.
  • When in doubt, verify with the reverse direction — mm ÷ 25.4 should return your original inch value.
  • In CAD and 3D printing, always confirm the document unit is mm before importing STL files.

Часто задаваемые вопросы

How many mm in an inch?

There are exactly 25.4 millimeters in 1 inch. To convert inches to millimeters, multiply the inch value by 25.4 — for example, 2 inches = 2 × 25.4 = 50.8 mm.

What is 3/8 inch in mm?

3/8 inch equals 9.525 mm. The exact calculation is 3/8 × 25.4 = 9.525 mm, commonly rounded to 9.53 mm for most practical work. 3/8" is a very common fastener and wrench size.

What is 5/16 inch in mm?

5/16 inch equals 7.9375 mm, usually rounded to 7.94 mm. The exact conversion is 5/16 × 25.4 = 7.9375 mm. 5/16" is a standard UNC bolt and wrench size.

What is 1 inch in mm?

1 inch is exactly 25.4 mm. This value is the international definition of the inch adopted in 1959 and used for all scientific and industrial conversions.

How do you convert inches to millimeters?

Multiply the inch value by 25.4: d(mm) = d(in) × 25.4. For example, 5 inches = 5 × 25.4 = 127 mm, and 20 inches = 20 × 25.4 = 508 mm.

How many inches are in a millimeter?

One millimeter equals approximately 0.03937 inches. To convert mm to inches, divide the millimeter value by 25.4 — for example, 10 mm ÷ 25.4 = 0.394 inches.

Need a complete fastener specification table for your project? Contact GUXIANG — we supply inch and metric fasteners with full dimensional data.
Отказ от ответственности: This page is for informational purposes only. Conversion values are calculated using the international definition 1 inch = 25.4 mm. GUXIANG makes no guarantees regarding the completeness or suitability of this information for specific applications; always verify critical dimensions against official standards.

Сопутствующие инженерные ресурсы

Редакция Guxiang Metalwork

Более 12 лет в производстве крепежных изделий. Мы специализируемся на стандартных и нестандартных крепежных изделиях, гайках, пружинах и шайбах, включая холодную высадку, накатку резьбы, механическую обработку и штамповку. Наше предприятие соответствует стандарту ISO 9001. & Сертифицирован по стандарту IATF 16949 и предлагает услуги OEM/ODM по всему миру.

Оглавление

Отправить ваш запрос
Делиться:
Вам также может понравиться
Калькулятор-скорости-сжатия-пружины-жесткости-img
Калькулятор веса крепежа & Таблицы веса
Размер шайбы & Таблица размеров толщины | САЭ & Военный корабль США
Таблица преобразования шкалы твердости HB HRC HV
Конвертер прочности на разрыв фунтов на квадратный дюйм в МПа
Таблица прочности маркировки болтов