Structural Fasteners

for Load and Weathering

Fasteners for steel frames, bridges, cladding systems and precast connections, in grade 8.8 and 10.9 steel with hot dip galvanizing and zinc flake coatings. Preload and slip critical behaviour specified with the joint, not after it.

8.8 · 10.9
Property classes per ISO 898-1
Preload control
Turn of nut, DTI and tension methods
HDG and zinc flake
Weathering protection systems
Slip critical aware
Coating and faying surface specified together
24 h
Inquiry response with lead time
Applications

Structural Fastener Applications

A structural joint is designed around the connection, not around the bolt. Whether the connection is bearing type or slip critical changes the specification completely, and getting it wrong is a design error rather a procurement one. These six assemblies are where that distinction matters.

Steel frame

Steel Structures and Building Frames

Design driver

Whether the joint is bearing type or slip critical. A slip critical joint cannot be coated on the faying surface at all.

Our approach

Grade and coating selected with the connection type in mind, and thread fit confirmed where hot dip galvanizing is used.

Typical parts Hex bolts, structural nuts, hardened washers, HSFG assemblies

Bridge structure

Bridges and Pedestrian Structures

Design driver

Fatigue under cyclic traffic loading, plus a corrosion allowance over the design life with no maintenance access.

Our approach

Coating system matched to the exposure, and material certificates that support the design life calculation.

Typical parts Structural bolts, shear connectors, bearing and expansion joint hardware

Cladding system

Cladding and Facade Systems

Design driver

Visible fasteners that must not stain the facade, and brackets that carry wind load into the structure.

Our approach

Stainless and coated systems selected so staining does not migrate onto the surrounding surface.

Typical parts Facade fasteners, bracket bolts, self drilling screws, rivet nuts

Roof system

Roof and Wall Systems

Design driver

Self drilling into thin sheet without distorting the thread, and a coating that survives being drilled.

Our approach

Self drilling geometry matched to the sheet gauge, with coatings that retain protection at the drilled edge.

Typical parts Self drilling screws, stitching screws, insulation fasteners, roof bolts

Falsework

Formwork and Falsework

Design driver

Repeated assembly and stripping cycles, so the fastener is reused many times and must not strip the thread.

Our approach

Thread form and grade chosen for reuse, with hard washers that do not brinell under preload.

Typical parts Wing nuts, tie rod components, clamp bolts, reusable thread bar

Precast connection

Precast Concrete Connections

Design driver

Cast in hardware that has to be located accurately before the pour and stay aligned afterwards.

Our approach

Machined cast in parts with locating features, supplied with dimensional reports for the setting out.

Typical parts Cast in sockets, anchor channels, lifting anchors, connection plates

Why GUXIANG

Why Structural Buyers Work with GUXIANG

We manufacture rather than trade, so forming, threading, heat treatment and finishing sit inside one facility. On a structural part that matters because the coating thickness, the thread fit and the material certificate all have to agree with each other, and a handover between suppliers is where that agreement usually breaks.

01

Connection type respected

Bearing type and slip critical joints are specified differently, and the difference is a design decision rather than a purchasing preference. We ask which one you have before quoting.

Slip critical and bearing joints quoted separately

02

Thread fit with HDG

Hot dip galvanizing adds zinc to both threads, so the tap is sized for the coating rather than for the bare thread. Confirmed before production, not at assembly.

Oversize tapping or masking agreed in advance

03

Preload method matched

Turn of nut, calibrated wrench and direct tension indicator washers each suit different joints. We supply the hardware that matches the method your specification calls for.

DTI washers and calibrated hardware available

04

Weathering systems selected by site

Coating systems are selected against the corrosivity category of the actual site rather than against a generic outdoor specification.

ISO 12944 category used to select the system

Not sure whether your joint is bearing type or slip critical?

Send the connection detail or the drawing reference. We will identify the connection type, confirm whether the faying surface can be coated, and flag the thread fit if hot dip galvanizing is specified.

Property Classes and Preload Control

A structural bolted joint is controlled by preload, not by bolt strength. Two methods are used in practice, and which one applies changes both the hardware and the inspection regime.

MethodHow preload is achievedVerificationNote
Snug tightenedNut run down to contact the pliesVisual, plus specified rotationBearing type joints only, no designed preload
Turn of nutSnug, then a specified further rotationRotation angle recordedSimple, needs consistent snug tightness
Calibrated wrenchTorque applied with a calibrated toolTorque value recordedFriction dependent, wide scatter on coated threads
Direct tension indicatorWasher deforms at target loadGap measured with a feeler gaugeMost reliable on site, independent of friction
Tensioning deviceHydraulic stretching of the boltLoad displayed on the deviceLarge diameters, high accuracy

Preload method should follow the connection design and the project specification rather than availability on site. A calibrated wrench gives poor repeatability on coated threads because friction varies between batches and between positions, which is why direct tension indicator washers are often specified where the preload is critical.

Coatings for Structural and Outdoor Service

Structural coatings are selected by the corrosivity category of the site and by whether the joint is slip critical. The same coating that protects a bearing joint can destroy a slip critical one.

SystemCorrosion classFaying surfaceThread fit affectedTypical use
Hot dip galvanizingVery highMust be masked if slip criticalYes, tap oversizeCoastal structural, long life
Zinc flake, non electroVery highCan be specified to a slip classMinimalBridges, slip critical joints
Dacromet / GeometVery highCan be specified to a slip classMinimalOffshore and coastal steelwork
Zinc nickelHighNot for slip criticalMinimalFacade and cladding hardware
Zinc aluminium mechanically platedHighCan be specified to a slip classMinimalStructural fasteners
Stainless, uncoatedStainless baseNot applicableNot applicableFacade and architectural

A slip critical connection cannot be coated on the faying surface. Slip resistance depends on a defined coefficient of friction between the connected plies, and any coating on that surface changes the coefficient and can eliminate the slip capacity the connection was designed for. Coatings are applied to the bolt, the nut and the washer, and the faying surface is left clean and uncoated unless the design explicitly specifies a friction class coating. If a slip critical joint is galvanized over the whole assembly, the connection has to be redesigned, not just recoated.

Documentation

Traceability and Documentation

Structural supply requires the material certificate chain and the coating records, because both feed the design calculation. Here is what can accompany an order.

Documentation available with your order

Traceability runs from the incoming mill certificate through forming, heat treatment and finishing, and is recorded by lot. Where your specification calls for a particular certificate format or a slip coefficient test, send the requirement with the enquiry so we can confirm it before production.

Commercial

Delivery and Trade Terms for Structural Buyers

The questions structural buyers ask before approving a new supplier, answered before you ask them.

Lead time, stock items
3 to 5 working days
Lead time, custom parts
15 to 25 working days after drawing approval
Prototype quantity
Single piece accepted, shipped by air freight
Volume shipping
Sea freight, LCL or FCL
Minimum order quantity
Flexible for machined parts, negotiable for fasteners
Packaging
Neutral, lot marked, labeled to your part number
Payment terms
T/T and L/C at sight, negotiable for established accounts
Incoterms
EXW, FOB, CIF, DAP
Technical FAQ

Structural Fastener FAQs

Answers to the questions structural engineers and procurement teams ask most often, with specific values rather than general assurances.

What is the difference between a bearing type and a slip critical joint?

A bearing type joint transfers load by shear and bearing on the bolt and the plate, and the bolts only need to be snug tightened. A slip critical joint transfers load by friction between the connected plies, which requires a designed preload and a controlled coefficient of friction on the faying surface. The two are not interchangeable, and the specification of the hardware and the inspection regime follow from which one the connection is designed as.

Not over the faying surface. Slip resistance depends on a defined coefficient of friction between the plies, and a coating on that surface changes the coefficient and can remove the slip capacity the connection was designed for. The bolt, nut and washer are coated, and the faying surface is left clean and uncoated unless the design explicitly specifies a coating qualified to a slip class. Zinc flake and mechanically plated systems can be supplied to a slip class, which is why they are often used on slip critical connections.

Yes. Zinc adds roughly 50 to 100 microns per surface, on both the male and the female thread, so a nut that fits on the bare thread will not assemble afterwards. The parts are either tapped oversize after galvanizing or the threads are masked during the process, and which approach applies should be agreed before the order. This is a common source of site delays when it is discovered during assembly rather than at the enquiry stage.

Direct tension indicator washers are the most reliable on site because they verify the load directly and are not affected by friction variation. Turn of nut is simple and inexpensive but depends on a consistent snug tightness. A calibrated wrench is convenient but gives poor repeatability on coated threads, because friction varies between batches and between positions in the same joint. Follow the project specification where one exists, and use DTI washers where the preload is critical.

Grade 8.8 covers most general structural work, and grade 10.9 is used where a higher preload or a smaller fastener is needed. The grade alone does not make the joint safe, because the connection capacity also depends on the plate, the end distance, the edge distance and the preload. Send the connection detail and we will confirm the grade and the hardware rather than quoting from the bolt size alone.

On structural connections the usual answer is designed preload rather than a locking device, because a properly preloaded joint does not loosen under transverse vibration the way a snug tightened one does. Where preload is not achievable or the joint is subject to impact, a prevailing torque locking element or a mechanical locking device is used. A structural lock washer is generally not sufficient on its own for a joint that sees cyclic loading.

High strength friction grip assemblies, meaning the bolt, nut and hardened washer supplied as a matched set, are available. The set matters because the washers are hardened to avoid brinelling under preload, and brinelling is one of the mechanisms that causes preload loss over time. If your specification calls for a matched assembly, say so at the enquiry so the washers are included in the quotation.

As a rule of thumb, one to one and a half times the nominal diameter of engagement in steel gives full bolt strength in most structural materials. Engagement is reduced where the mating material is weaker, and increased where it is aluminium or a soft casting. For structural connections the engagement is usually set by the plate thickness and the connection design rather than chosen freely, so confirm against the connection detail.

An EN 10204 3.1 material certificate with heat lot traceability, a dimensional inspection report, a mechanical property test report and coating thickness measurement. Slip coefficient test reports are available on request where the connection is slip critical. Where your specification calls for a particular certificate format, send the requirement with the enquiry so we can confirm it before production.

Yes. Construction projects often need moderate quantities of many different parts, and single piece prototypes are accepted for machined components and cast in hardware. Low volume changes the unit cost, so the price per part will be higher than a repeat production run, but we quote the job as it is. Samples ship by air freight.

Request a quote

Send a Connection Detail or Drawing

One message is enough. A connection detail, a drawing reference, or a plain description of the joint is enough for us to start.

  • Reply within 24 hours on working days
  • Connection type confirmed before quoting
  • Material certificate and coating records with supply
  • Slip coefficient testing available on request
Do you have the drawings?
Related categories and resources