  1. Performance & Material Properties
    • Alloy Steel Construction: Bodies machined from quenched‐and‐tempered 4140 alloy steel (tensile strength up to ≈800 MPa, hardness 40–45 HRC) for maximum fatigue and shear resistance.
    • Hardened Ball & Spring: High-precision bearing steel ball (≈RC 55–60) captured on a spring tempered to deliver consistent preload forces (5–30 N, depending on size).
    • Protective Finish: Standard zinc-nickel plating (8–12 µm) or black-oxide coating for corrosion protection and reduced galling in industrial environments.
  2. Detailed Application Range
    • Indexing & Positioning: Provide positive “click‐stop” detents in jigs, fixtures, rotary tables, machine tool slides and assembly stations for repeatable location.
    • Locking & Latching: Secure panels, doors, drawers and movable guards in automation cells, packaging machinery and medical equipment.
    • Component Holding: Apply constant preload on sensors, optical mounts, circuit-board holders, and end-effector attachments in robotics and instrumentation.
    • Assembly & Conveyance: Guide workpieces into precise stops on conveyors, stamping presses, textile machines and material-handling systems.
  3. Effortless Installation & Adjustment
    • Internal Hex Drive: Recessed 2 mm–8 mm Allen socket ensures slip-free engagement and controlled torque (up to 15 Nm) for rapid insertion and withdrawal.
    • Self-Contained Spring Mechanism: No external spring or detent plate required—built-in spring retains the ball and provides uniform force throughout its travel.
    • Quick Servicing: Standard threaded body (M3–M12) screws in and out cleanly; ball assembly can be disassembled for cleaning or replacement without special tools.
  4. Superior Quality & Long-Term Reliability
    • Precision Manufacturing: Produced in ISO 9001-certified facilities to DIN 1481/1480 tolerances (±0.1 mm on thread OD, ±0.05 mm on ball diameter) for interchangeability.
    • Rigorous Testing: Each lot undergoes ball-preload measurement, dimensional inspection and corrosion testing (240 h salt-spray per ASTM B117) to ensure consistent performance.
    • Full Traceability & Compliance: Material certification from melt lot to finished part; RoHS-compliant and free of magnetic anomalies—guaranteeing dependable operation in the most demanding applications.

Additional information

Coating

Black, color customizable

Diameter

M3, M4, M6, M8, M10, M12, M14, M18, 1/4-20, 10#-24, 10#-32, 5/16-18, 8#-32

Length

1-1/2, 1-1/4, 1-3/4, 1'', 1/2, 100, 110, 16, 20, 25, 3/4, 3/8, 30, 35, 40, 45, 5/8, 50, 60, 7/8, 70, 80, 85

Manufacturer

GUXIANG

Material

Alloy Steel, Carbon Steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province