Compression Spring, Spring Steel Construction Wire Diameter 0.3-2mm Outer Diameter 3-40mm spring steel Description

  1. Performance
    • High-Carbon Spring Steel Construction – Coiled from DIN EN 10270-1 grade SH or ASTM A228 (music wire) with tensile strengths between 1 600–2 000 MPa depending on wire diameter (Ø0.3–2 mm). The steel is oil-tempered and stress-relieved at 250 °C, yielding long-cycle elasticity and minimal permanent set.
    • Broad Dimensional Range – Standardised outer diameters Ø3–40 mm and free lengths up to 200 mm cover light tactile push-buttons through to heavy machine linkages. Spring rates span 0.05–35 N mm⁻¹, enabling precise load matching.
    • Shot-Peened & Polished Surface – Compressive residual stresses from shot peening boost fatigue life by 30–50 %. Fine-polish finish (Ra ≤ 0.8 µm) reduces friction in tight guide bores and mitigates corrosion initiation points.
    • Operating Window – Reliable force delivery from −40 °C to +120 °C; modulus varies <3 % across this range, ensuring consistent performance in outdoor, automotive, and electronics environments.
  2. Application Scenarios & Assembly Requirements
    • Precision Mechanisms – Keyboards, microswitches, camera shutters, and medical dispensers employ the Ø0.3–0.6 mm series for crisp tactile response and controlled return forces.
    • Industrial & Automotive – Ø1.0–2.0 mm models act as valve train followers, latch actuators, and vibration isolators where high cycle counts (>10⁶) and compact envelopes are mandatory.
    • Assembly Guidelines –
    – Housing clearance: inner guide diameter = spring OD + 0.15 × wire Ø to prevent side-load buckling.
    – Maximum deflection: limit working stroke to 80 % of solid height to preserve ≥95 % load after 100 000 cycles.
    – End treatment: ground and closed ends offer <3° squareness for even load distribution; unground ends suit low-precision pockets.
    • Pre-Set Option – Factory scragging eliminates early relaxation, allowing designers to use published load values without additional settling allowances.
  3. User-Friendly Operation
    • Color-Coded Identification – Each spring is epoxy-tipped in industry-standard colors corresponding to rate and wire diameter, simplifying on-site selection and reducing assembly errors.
    • Ready-to-Install Packaging – Springs are supplied lightly oiled in anti-static trays; quantities ≤500 pcs arrive on continuous strips for automated pick-and-place feeders, while larger diameters are banded in nested stacks to avoid tangling.
    • Tool-Free Fitment – Smaller sizes compress easily by finger pressure; larger units require only a simple compression sleeve or bench vise—no special mandrels or jigs.
    • Dimensional Trace Codes – Laser-etched batch numbers on the last coil link to online datasheets for real-time load/deflection curves and CAD models, streamlining maintenance documentation.
  4. Quality & Longevity
    • ISO 9001 & IATF 16949 Certified Manufacturing – Statistical process control on coil pitch, heat treatment, and surface integrity ensures force tolerance within ±7 % and free-length tolerance within ±1 mm.
    • Fatigue & Load-Relaxation Validation – Sample springs endure 1 000 000 compression cycles at 60 % solid height with force loss <5 %, and exhibit <2 % relaxation after 48 h at 100 °C.
    • Corrosion Protection & Compliance – Optional zinc-phosphate or black oxide coatings provide >72 h neutral salt-spray resistance without affecting spring rate. All materials are RoHS and REACH conformant, free from Cr⁶⁺ and other restricted substances.
    • Comprehensive Documentation – Each shipment includes a 3.1 material certificate and test report covering tensile strength, surface roughness, dimensional checks, and residual stress measurements, assuring predictable, long-term service in safety-critical assemblies.

Additional information

Wire Diameter(mm)

0.3, 0.4, 0.5, 0.7, 0.8, 0.9, 1.0, 1.2, 1.4, 1.5, 1.6, 1.8, 2.0, 2.5, 3.0, 4.0, 5.0

Spring Outer Diameter(mm)

10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 2, 20, 22, 24, 25, 28, 3, 30, 32, 35, 38, 4, 40, 42, 45, 5, 50, 55, 6, 62, 7, 8, 9

Spring Length(mm)

200, 300

Material

Spring steel

Manufacturer

GUXIANG

Shipping Term

EXW Guangdong Province

Package Size(cm)

30*20*20