Carbon Steel Internal Circlips Snap Retaining Ring Description

  1. Robust, Versatile Retention Performance
    • Cold-formed from high-carbon or alloy spring steel (65 Mn / 51CrV4) and austempered to ≥ 1 000 MPa tensile strength, each internal circlip delivers steady radial spring pressure that keeps bearings, gears and seals locked in their housing grooves under thrust loads above 3 kN and circumferential speeds to 25 m s⁻¹.
    • A ≥ 8 µm electro-zinc layer with trivalent chromate passivation protects the metal from red-rust corrosion for at least 120 h neutral-salt-spray; duplex systems (zinc + epoxy) extend endurance beyond 1 000 h and can be supplied in clear, yellow, black, olive or any RAL / Pantone shade without altering spring behaviour.
    • Shot-peen conditioning introduces compressive residual stress, boosting fatigue life past 10⁶ load cycles, while deburred lug holes and rounded edges reduce tool wear and eliminate stress-risers.
    • Stable over −50 °C … +200 °C, the rings maintain preload after thermal cycling or vibration, making them a compact alternative to threaded retainers where axial space is tight.
  2. Broad, Cross-Industry Application Spectrum
    • Automotive & Mobility: Locks wheel-hub bearings, synchroniser hubs and motorcycle clutch baskets that see oil splash, road salt and high RPM.
    • Industrial Power-train & Robotics: Secures spur gears, needle bearings and seals inside servo gearboxes, conveyors and packaging machinery subject to wash-downs and dynamic loading.
    • Construction, Mining & Agricultural Equipment: Prevents shaft components from drifting in hydraulic pumps, track-roller assemblies and PTO couplings exposed to shock and grit.
    • HVAC, Renewable Energy & Marine: Retains fan spacers, turbine rotor sleeves and valve seats in chillers, wind turbines and desalination units facing chloride attack, temperature swings and vibration.
  3. Installer-Friendly, Time-Saving Handling
    • Standard lug holes accept straight- or angled-tip snap-ring pliers; a single compress-and-release action drops the ring into its groove—no screws, shims or thread locking compounds required.
    • Radial flexibility accommodates typical H9 bore tolerances, so housings need only conventional machining accuracy, reducing secondary operations and on-site rework.
    • Colour-coded plating and optional laser-etched diameter codes enable instant size identification during kitting or robotic feed, cutting assembly cycle time.
    • Rings are supplied lightly oiled and nested in tear-proof, resealable pouches that keep parts tangle-free and ready for line-side use or field maintenance kits.
  4. Certified Quality & Long-Term Durability
    • 100 % optical and laser-gauge inspection confirms free diameter ±0.03 mm, groove thickness ±0.02 mm, flatness ≤0.05 mm and lug symmetry; Cp/Cpk ≥ 1.67 data are archived under ISO 9001 and IATF 16949 quality systems.
    • Accelerated ageing—500 h cyclic humidity, 100 freeze-thaw cycles and 2 × 10⁶ vibration pulses at 70 % proof load—shows ≥ 95 % retained radial spring force with zero coating delamination or cracking.
    • Lot-level QR codes link every ring to melt chemistry, heat-treat curve, coating batch and dimensional record, providing full traceability for safety-critical applications.
    • Compliance with RoHS and REACH ensures the rings are free from restricted substances, while the maintenance-free zinc surface eliminates the need for periodic re-lubrication in service.

Additional information

Coating

Black, color customizable

Diameter

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

Manufacturer

GUXIANG

Material

Alloy Steel, Carbon Steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces