  1. Robust, Versatile Retention Performance
    • Cold-formed from high-carbon or alloy spring steel (65 Mn / 51CrV4) and austempered to ≥ 1 000 MPa tensile strength, each internal circlip delivers steady radial spring pressure that keeps bearings, gears and seals locked in their housing grooves under thrust loads above 3 kN and circumferential speeds to 25 m s⁻¹.
    • A ≥ 8 µm electro-zinc layer with trivalent chromate passivation protects the metal from red-rust corrosion for at least 120 h neutral-salt-spray; duplex systems (zinc + epoxy) extend endurance beyond 1 000 h and can be supplied in clear, yellow, black, olive or any RAL / Pantone shade without altering spring behaviour.
    • Shot-peen conditioning introduces compressive residual stress, boosting fatigue life past 10⁶ load cycles, while deburred lug holes and rounded edges reduce tool wear and eliminate stress-risers.
    • Stable over −50 °C … +200 °C, the rings maintain preload after thermal cycling or vibration, making them a compact alternative to threaded retainers where axial space is tight.
  2. Широкий, межотраслевой спектр применения
    • Automotive & Mobility: Locks wheel-hub bearings, synchroniser hubs and motorcycle clutch baskets that see oil splash, road salt and high RPM.
    • Industrial Power-train & Robotics: Secures spur gears, needle bearings and seals inside servo gearboxes, conveyors and packaging machinery subject to wash-downs and dynamic loading.
    • Construction, Mining & Agricultural Equipment: Prevents shaft components from drifting in hydraulic pumps, track-roller assemblies and PTO couplings exposed to shock and grit.
    • HVAC, Renewable Energy & Marine: Retains fan spacers, turbine rotor sleeves and valve seats in chillers, wind turbines and desalination units facing chloride attack, temperature swings and vibration.
  3. Установщик-дружественный, экономящий время
    • Standard lug holes accept straight- or angled-tip snap-ring pliers; a single compress-and-release action drops the ring into its groove—no screws, shims or thread locking compounds required.
    • Radial flexibility accommodates typical H9 bore tolerances, so housings need only conventional machining accuracy, reducing secondary operations and on-site rework.
    • Colour-coded plating and optional laser-etched diameter codes enable instant size identification during kitting or robotic feed, cutting assembly cycle time.
    • Rings are supplied lightly oiled and nested in tear-proof, resealable pouches that keep parts tangle-free and ready for line-side use or field maintenance kits.
  4. Сертифицированное качество и долговечность
    • 100 % optical and laser-gauge inspection confirms free diameter ±0.03 mm, groove thickness ±0.02 mm, flatness ≤0.05 mm and lug symmetry; Cp/Cpk ≥ 1.67 data are archived under ISO 9001 and IATF 16949 quality systems.
    • Accelerated ageing—500 h cyclic humidity, 100 freeze-thaw cycles and 2 × 10⁶ vibration pulses at 70 % proof load—shows ≥ 95 % retained radial spring force with zero coating delamination or cracking.
    • Lot-level QR codes link every ring to melt chemistry, heat-treat curve, coating batch and dimensional record, providing full traceability for safety-critical applications.
    • Compliance with RoHS and REACH ensures the rings are free from restricted substances, while the maintenance-free zinc surface eliminates the need for periodic re-lubrication in service.

Дополнительная информация

Покрытие

Черный, цвет настраиваемый

Диаметр

1.6, 10, 12, 16, 18, 20, 22, 24, 27, 30, 32, 36, 45, 48, 50, 6, 8

Производитель

GUXIANG

Материал

Сплавная сталь, углеродистая сталь

Размер упаковки (см)

30*20*20

Условия доставки

EXW провинция Гуандун

Артикул

1 000 000 штук

Связанные с товаром