304 Stainless Steel Torx Pan Head Self Tapping Wood Screw

SKU N/A Category

Quantity

Unit Price

Price

Price range: $0.021 – $0.030

Price range: $0.021 – $0.030

Total:

Price range: $0.021 – $0.030

304 Stainless Steel Torx Pan Head Self Tapping Wood Screw Description

304 Stainless Steel Torx Pan Head Self Tapping Wood Screw

1.Superior Corrosion Resistance & Mechanical Strength
Machined from 18-8 (304) stainless steel, these pan-head wood screws deliver a tensile strength of ≈515 MPa and yield strength of ≈205 MPa, with a hardness of ~80 HRB. The fully passivated, polished finish resists rust, oxidation and most chemicals—ideal for both indoor and outdoor joinery.

2.Versatile Wood & Composite Applications
Engineered for fastening hardwoods, softwoods, plywood, MDF and composite decking. The large pan head provides a broad bearing surface for secure clamping in cabinetry, furniture assembly, exterior trim, marine joinery and playground equipment.

3.Precision Torx Drive & Self-Tapping Design
The recessed Torx (T15–T25) socket ensures self-centering engagement and high torque transfer (up to 12–15 Nm) with virtually no cam-out. Combined with a Type-17 self-tapping point and optimized coarse thread, these screws pierce and hold firmly without pre-drilling, speeding installation and reducing wood splitting.

4.Certified Quality & Long-Lasting Reliability
Produced in ISO 9001-certified facilities to ANSI B18.6.1 tolerances (±0.1 mm). Each batch undergoes dimensional inspection, drive-torque testing and ≥240 h salt-spray per ASTM B117. Full material traceability and RoHS compliance ensure consistent, enduring performance.

Additional information

Coating

Plain

Drive Type

Torx Drive

Head Type

Pan Head

Diameter

ST4.2, ST4.8, ST5.5

Length

16, 19

Manufacturer

GUXIANG

Material

Stainless steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU