description
- Performance & Material Properties
• DIN 508 Extended T-Nut Design – Manufactured to DIN 508 dimensions, these extended T-nuts feature a longer body for increased thread engagement and two anti-rotation prongs that embed into the slot base, delivering up to 25 % greater pull-out strength versus standard T-nuts.
• High-Strength Carbon & Alloy Steel Options – Forged from C45 carbon steel or optional 42CrMo4 alloy steel, quenched and tempered to achieve tensile strengths of 600–900 MPa and Rockwell hardness HRC 30–45.
• Precision Threads – Cold-rolled metric threads (M6–M12) to ISO 965/1 class 6H tolerances (±0.1 mm) for burr-free engagement, smooth torque curves and >10 000 assembly cycles without galling or stripping.
• Black Oxide & Custom Color Finishes – Standard black‐oxide conversion coating provides ≥72 h salt-spray resistance (ASTM B117) and low reflectivity. Optional epoxy‐polyester powder‐coating in any RAL color adds UV stability, abrasion resistance and visual part coding. - Detailed Application Range
• Heavy-Duty Framing & Structural Assemblies – Ideal for industrial machine frames, safety barriers, mezzanine platforms and workbenches using 8–16 mm wide T-slots.
• Renewable Energy & Solar Mounting – Secures photovoltaic racking rails, inverter brackets and cable trays on aluminum profiles in outdoor installations.
• Automation, Robotics & Conveyor Systems – Fastens linear guides, sensor mounts, guard panels and chain guides on production lines, pick-and-place machines and AGV docking stations.
• Modular Fixtures & Display Racks – Builds adjustable retail shelving, trade-show exhibits, shop-fitting walls and custom furniture where frequent reconfiguration and aesthetic finish matter. - Effortless Operation & User Convenience
• Drop-In & Slide-In Installation – Simply insert the extended T-nut into the slot opening; the anti-rotation prongs dig in to hold it upright so you can slide to any position before fastening—no end-feed plates or sideways entry required.
• Rapid Repositioning & Maintenance – Loosen the bolt slightly to disengage the prongs, slide the nut to a new location and retighten—enabling quick layout changes or maintenance without dismantling the frame.
• Universal Tool Compatibility – Works with standard hex keys, deep-well sockets, impact drivers and torque wrenches; no special tooling or adapters needed.
• Ready-To-Use Kits & Bulk Packaging – Offered by Amazon, McMaster-Carr, Misumi, RS Components, Fastenal and Grainger in assorted M6–M12 packs (50–500 pcs) with matching screws and clear compartment trays for efficient inventory management. - Superior Quality & Long-Term Reliability
• Certified & Traceable Manufacturing – Produced in ISO 9001 and ISO 14001 facilities to DIN 508 and ANSI/ASME B18.2.2 standards, ensuring consistent dimensions, thread accuracy and material grade traceability.
• Rigorous Testing Protocols – Each batch undergoes ≥72 h salt-spray (ASTM B117), 5 000 torque-to-turn cycles and ultrasonic inspection to verify coating adhesion, thread integrity and fatigue life.
• Vibration & Shock Resistance – Anti-rotation prongs and chamfered T-head edges prevent loosening under dynamic loads, vibration and thermal cycling (–40 °C to +120 °C).
• Environmental & Safety Compliance – RoHS- and REACH-compliant; free of hexavalent chromium and other restricted substances, delivering decades of corrosion-resistant, maintenance-free service in even the harshest industrial and coastal environments.