Acorn Cap Nut-Carbon Steel Acorn Cap Dome Head Nut Description

  1. Solid Mechanical Performance
    • Cold-forged from medium-carbon steel and heat-treated to Class 8 (≈ 800 MPa tensile), these DIN 1587 acorn cap nuts deliver high clamp loads without thread shear in structural steel, aluminium, or timber joints.
    • A duplex finish—8 µm electro-zinc plus trivalent-chromate passivation—provides baseline 120 h neutral-salt-spray protection; optional colour powder-coat or nylon-patch locking rings boost corrosion life beyond 500 h and add vibration resistance.
    • The seamless domed cap fully encloses protruding male threads, guarding against impact, snagging, and galvanic corrosion in mixed-metal assemblies.
  2. Broad, Cross-Industry Application Spectrum
    • Furniture & Playground Equipment: Creates a smooth, child-safe termination on exposed bolts in flat-pack cabinetry, fitness rigs, and outdoor play structures.
    • Automotive & Powersports: Caps chassis, suspension, and engine studs, combining cosmetic flair with rust prevention in wheel wells, battery trays, and exhaust hangers.
    • Construction & Solar Frames: Secures guard-rail brackets, façade clips, and photovoltaic modules where weatherproofed hardware is mandatory.
    • OEM Machinery & Appliances: Offers a hygienic, easy-clean bolt finish on guard doors, agitator housings, and consumer devices—compatible with spray-paint colour matching for corporate branding.
  3. Fast, Operator-Friendly Handling
    • Standard hex drive mates with any metric or imperial socket; the domed cap removes the need for separate finishing washers, cutting assembly time by up to 25 % on production lines.
    • Light interference fit on the first thread lets technicians start nuts by hand—even in overhead or blind-stud positions—reducing cross-thread risk and tool fatigue.
    • Available in loose bulk, resealable bags, or tape-and-reel formats stocked for seamless integration into manual stations or automated pick-and-place feeders.
  4. Premium Quality & Customisable Aesthetics
    • 100 % vision inspection validates cap concentricity ≤ 0.03 mm TIR and burr height < 0.05 mm; SPC data can be supplied for ISO 9001, IATF 16949, or PPAP Level 3 audits.
    • Colour options include RAL/Pantone powder coats, black oxide with micro-crystalline wax, or nickel-chrome decorative plating—ideal for brand coding, maintenance-zone tagging, or high-end consumer finishes.
    • Every carton ships with RoHS 3, REACH, and DFARS material certificates plus a QR code linking to melt-lot traceability, satisfying aerospace, medical-device, and food-equipment supply-chain requirements.

Additional information

Coating

Blue Zinc, color customizable

Diameter

M3, M4, M6, M8, M10, M12, M14, M18, 1/4-20, 10#-24, 10#-32, 5/16-18, 8#-32

Manufacturer

GUXIANG

Material

Stainless steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces