Sealing Washer 304 Stainless Steel Neoprene EPDM Bonded Neoprene Rubber Washers Gasket Description
- Reliable, Weather-Tight Sealing Performance
• The washer combines a 304 stainless-steel backing cup with co-molded Neoprene or EPDM elastomer, creating a single, bonded unit that compresses evenly under torque to form a long-life, leak-free gasket.
• 304 stainless provides ≥ 18 % Cr / 8 % Ni corrosion resistance, while the elastomer remains pliable from −40 °C to +120 °C (Neoprene) or −50 °C to +150 °C (EPDM), shrugging off UV, ozone, salt spray, and mild acids.
• A raised, concentric sealing ridge on the rubber faces the joint surface; under recommended torque it yields 15–25 % compression set, blocking water, oil, and compressed air up to 1.6 MPa without cold-flow or creep.
• Stainless cup edge rolls over the rubber shoulder, shielding the polymer from mechanical damage and enabling >1 000 h neutral salt-spray endurance with no red rust or galvanic staining. - Широкий спектр межотраслевых приложений
• Architectural Roofing & Facades: Seals self-drilling screws on metal roofing sheets, curtain-wall mullions, and solar-panel rails exposed to driving rain and daily temperature cycles.
• HVAC, Plumbing & Fire-Protection Systems: Prevents leakage around sheet-metal duct screws, sprinkler hangers, and water-heater jackets that undergo thermal expansion and vibration.
• Автомобильная, морская промышленность & Rail Vehicles: Maintains watertight joints in body panels, lighting housings, and deck hardware subjected to road salt, spray, and continuous flexing.
• Electronics Enclosures & Renewable-Energy Cabinets: Provides IP-rated sealing for control boxes, junction covers, and inverter housings where gasket compression must remain stable over decades. - Удобство установки и экономия времени в обращении
• One-piece bonded design eliminates juggling separate metal and rubber parts; workers simply place the washer under any hex-head, sheet-metal, or self-tapping screw and drive to the standard torque.
• The stainless rim centers the fastener during spin-up, reducing run-out and stripping, while the rubber lip self-seats even on slightly irregular or painted substrates—ideal for field crews in variable conditions.
• Compatible with power drivers and automated feed systems; washers are available pre-assembled on screws or in bulk cartons for rapid line-side replenishment.
• Low added stack height (≤ 2 mm for #10 / M5 size) fits tight clearances without requiring longer fasteners or larger pilot holes, streamlining retrofits and repairs. - Проверенное качество & Долгосрочная долговечность
• Each batch undergoes 100 % visual and random hydraulic-pressure testing (sampled to ISO 2859-1) to ensure zero pinholes, bond voids, or cup cracks; typical Cp/Cpk ≥ 1.67 for critical dimensions.
• Elastomer hardness 50 ± 5 Shore A, tensile strength ≥ 7 MPa, and compression-set ≤ 25 % at 100 °C/22 h guarantee lasting elasticity; stainless hardness ≤ 200 HV prevents brittle failure during installation.
• Accelerated ageing trials—1 000 h UV exposure, 168 h salt-spray, and 500 thermal cycles from −40 °C to +90 °C—show no loss of sealing force or rubber-to-metal adhesion.
• Packaging features lot-coded labels linking melt chemistry, rubber compound certs, and test reports, providing traceability and confidence for safety-critical construction, transport, and industrial projects.