T Nut Roll in Spring T Nut with Spring Sheet Carbon Steel Nickel Plated for 2020 Series Slot Aluminum Profile Description
- Производительность & Свойства материала
• Высокопрочный углерод & Alloy Steel Core – Forged from C1045 carbon steel or optional 4140 chromoly alloy, quenched and tempered to deliver tensile strengths up to 900 MPa and Rockwell hardness HRC 40–45 for exceptional shear, pull-out and fatigue resistance.
• Precision M5 Thread & Spring-Sheet Retention – Cold-rolled threads to DIN 25201 tolerances (±0.05 mm) ensure burr-free engagement and >10,000 assembly cycles. A tempered 301-grade stainless leaf-spring snaps into the 6 mm slot wall of 2020 profiles, “roll-in” locking the T-nut in place during handling or vertical mounting.
• Nickel Plating & Color Customization – Standard trivalent nickel plating (8–12 µm) delivers ≥240 h neutral salt-spray resistance (ASTM B117). Optional epoxy-polyester powder-coat in any RAL color adds UV stability, scratch resistance and on-profile visual coding.
• Low-Profile T-Head Geometry – Compact 8 × 12 mm T-head slides smoothly into 6 mm slots, distributing clamp loads evenly to minimize slot deformation under torques up to 5 Nm. - Подробный диапазон применения
• Light-Duty Framing & Enclosures – Ideal for 2020 extrusion assemblies: machine guards, instrument housings, display cases and protective screens in workshops, laboratories and clean-rooms.
• Автоматизация & Hobby Robotics – Secures linear rails, sensor brackets, camera mounts and end-effector plates on desktop CNC mills, 3D printers, pick-and-place rigs and DIY robotic cells—enabling rapid prototyping and precise alignment.
• Модульные светильники & Retail Displays – Fastens shelving rails, LED signage tracks, tablet holders and countertop frames for trade-show exhibits, POS kiosks and adjustable office partitions.
• Лаборатория, Медицинская & Office Systems – Mounts monitor arms, cable management trays, instrument clamps and ergonomic accessories in lab benches, medical carts and sit-stand desks—environments demanding hygiene, corrosion resistance and tool-free adjustability. - Легкая работа & Удобство пользователя
• True Roll-In Installation – Drop the spring-sheet T-nut into any section of the 6 mm slot; it locks in place, allowing you to slide it to the exact mounting point before inserting and torquing the screw—no end-feed plates or rear access required.
• Quick-Shift Repositioning – Loosen the fastener partway to disengage the leaf spring, slide the nut to a new position, then retighten—enabling design tweaks or maintenance without full disassembly.
• Universal Tool Compatibility – Works with standard hex keys, deep-well sockets, impact drivers and torque wrenches; no proprietary tools or special adapters needed.
• Ready-To-Use Assortment Kits –mixed-size sets (50–200 pcs) with matching M5 screws and spring-sheet clips, organized in compartment trays or magnetic cases for on-site efficiency. - Превосходное качество & Долгосрочная надежность
• Сертифицированный & Traceable Manufacturing – Produced in ISO 9001 and ISO 14001 facilities to DIN 25201 and ANSI/ASME B18.2.2 standards, ensuring consistent geometry, thread accuracy and material integrity.
• Rigorous Testing Protocols – Every batch endures ≥240 h neutral salt-spray (ASTM B117), 10,000 torque-to-turn cycles and ultrasonic crack detection to verify plating adhesion, thread durability and retention performance.
• Вибрация & Ударопрочность – удержание листовой пружины и скошенные кромки Т-образной головки предотвращают вращение или ослабление при динамических нагрузках, вибрации и термоциклировании (от –40 °C до +120 °C).
• Относящийся к окружающей среде & Соответствие требованиям безопасности – соответствует требованиям RoHS и REACH; не содержит шестивалентного хрома и других запрещенных веществ. Сталь высокой чистоты, точная прокатка и равномерная обработка обеспечивают десятилетия необслуживаемой и устойчивой к коррозии эксплуатации даже в самых суровых промышленных или прибрежных условиях.