Din137 Carbon Steel Belleville Washer Conical Disc Spring Cup Washer

Artikelnummer k. A. Kategorie

Anzahl

Stückpreis

Preis

Preisspanne: $0.010 bis $0.045

Preisspanne: $0.010 bis $0.045

Gesamt:

Preisspanne: $0.010 bis $0.045

Din137 Carbon Steel Belleville Washer Conical Disc Spring Cup Washer Beschreibung

  1. Compact, High-Energy Spring Performance
    • Manufactured to DIN 137 Type A/B geometry from quenched-and-tempered carbon or alloy spring steel (65 Mn / 50CrV4), each conical disc converts minimal axial space into clamp forces of 0.4 – 4 kN at 75 % deflection, holding preload after joint relaxation, thermal cycling, or vibration.
    • ≥ 8 µm electro-zinc with trivalent passivation resists red rust for ≥ 120 h neutral-salt-spray; duplex finishes (zinc + epoxy powder) extend endurance to 1 000 h and can be tinted clear, yellow, black, olive, or any RAL/Pantone shade without altering spring rate or torque coefficient.
    • Cold-worked structure (≥ 1 000 MPa tensile) delivers repeatable load–deflection curves across −50 °C … +200 °C; shot-peen compression boosts fatigue life beyond 2 × 10⁶ cycles at 60 % deflection.
    • Polished contact bands (Ra ≤ 1.6 µm) and burr-free edges minimise friction scatter, enabling accurate torque-to-tension conversion with standard Class 8.8–12.9 fasteners.
  2. Vielseitig, branchenübergreifend Anwendung Spektrum
    • Automotive & Mobility: Maintains tension on brake-caliper brackets, exhaust couplings, and driveline shafts exposed to heat, vibration, and splash.
    • Industrial Machinery & Automation: Compensates for bearing settle, gasket creep, and frame expansion in gearboxes, servo mounts, and robotic end-effectors.
    • Construction & Heavy Equipment: Absorbs shock loads in boom pivots, crusher housings, and rail joints, preventing bolt loosening under impact.
    • Energy, HVAC & Electronics: Provides low-profile compliance in solar-panel clamps, turbine casings, inverter busbars, and PCB retainers subjected to daily temperature swings.
  3. Installateurfreundliches, zeitsparendes Handling
    • Drop-in replacement for flat M3–M24 washers—simply place the disc with the concave face toward the joint and torque to catalogue values; no shimming, lock nuts, or special tools required.
    • Shallow cone and low solid height fit tight stack-ups where coil springs cannot, enabling lighter assemblies and reduced envelope.
    • Oversized bore and entry chamfer speed manual or robotic insertion over painted or hot-dip-galvanised bolts; knurled or serrated variants add anti-slip bite for joints prone to micro-movement.
    • Supplied in resealable, stackable packs; laser-etched size and load markings plus optional colour-coded coatings simplify sorting, kitting, and on-site verification.
  4. Proven Quality & Long-Term Durability
    • 100 % dimensional inspection confirms OD ±0.05 mm, thickness ±0.02 mm, cone angle ±0.5°, and parallelism ≤0.03 mm; Cp/Cpk ≥ 1.67 data archived under ISO 9001, IATF 16949, and EN 1090 systems.
    • Accelerated ageing—500 h cyclic humidity, 100 freeze-thaw cycles, and 1 000 h UV exposure—shows ≥ 95 % preload retention with zero coating delamination.
    • Salt-spray, vibration, and thermal-shock tests validate suitability for coastal, desert, alpine, and industrial atmospheres without supplementary lubrication or maintenance.
    • Lot-level QR codes link each washer to melt chemistry, heat-treat curve, coating batch, and load-deflection record, giving engineers full traceability and confidence for safety-critical assemblies across industries.

Weitere Informationen

Beschichtung

Schwarz, Farbe individuell wählbar

Durchmesser

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

Hersteller

GUXIANG

Material

Legierter Stahl, Kohlenstoffstahl

Verpackungsgröße (cm)

30*20*20

Versandbedingungen

EXW Provinz Guangdong

Artikelnummer

1.000.000 Stück

Produktbezogen