DIN 5406 Carbon Steel Shaft Locking Washer Description
- High-Strength, Non-Reversible Locking Performance
• Manufactured to DIN 5406 dimensions from quenched-and-tempered alloy / carbon steel (typical hardness 38 – 46 HRC), the washer delivers the elasticity required for repeated bending of its locking tabs without cracking while preserving the tensile strength needed for heavy-duty shaft applications.
• The precision-lasered inner tongue keys into the shaft groove; one or two outer tabs are then bent into the nearest slots of the accompanying slotted nut, creating a fully mechanical lock that cannot unwind under shock, reversing torque, or thermal cycling.
• A ≥ 8 µm electro-zinc layer sealed by trivalent passivation shields the base metal for ≥ 120 h neutral salt-spray (ISO 9227); optional clear, yellow, black, olive, or custom RAL / Pantone top-coats extend corrosion life past 1 000 h while offering instant visual coding.
• Endurance testing shows ≥ 95 % retention of the original tightening torque after 1 000 000 torsional reversals at 50 Hz, confirming long-term reliability in demanding drive-train environments. - Branchenübergreifendes Anwendungsspektrum
• Kraftübertragung & Gearboxes: Locks KM / KML nuts on helical, bevel, and planetary gear sets inside conveyors, mixers, winders, and winches.
• Erneuerbare Energie, Marine & Rail: Secures bearing take-up nuts on yaw drives, propeller shafts, and axle journals that face pulsating loads, vibration, and outdoor weather cycles.
• Werkzeugmaschinen, Robotik & Precision Equipment: Maintains preload on high-speed spindles and ball-screw bearings, preserving micron-level accuracy during rapid acceleration.
• Bauwesen, Bergbau & Off-Highway Vehicles: Prevents nut walk-off on crusher shafts, drilling rigs, and hydraulic pump drives where downtime is costly and maintenance windows are brief. - Installateurfreundliche, zeitsparende Handhabung
• Assembly is straightforward: slide the keyed washer onto the shaft, torque the slotted nut to specification, then bend the closest tab into a nut slot with standard pliers—no adhesives, lockwire, or specialty fixtures.
• Chamfered tab edges reduce scoring when bent and allow one un-bend/re-bend cycle for maintenance without sacrificing grip, lowering consumable usage.
• Slim body thickness (1 – 3 mm across the size range) keeps bearing stacks compact, permitting drop-in retrofits without redesigning housings or altering cover depths.
• Supplied loose, in heat-numbered sachets, or on continuous tape for automatic dispensers; optional laser-etched size codes aid fast identification on multi-diameter assembly lines. - Zertifizierte Qualität & Langfristige Haltbarkeit
• 100 % in-process optical inspection verifies bore diameter, key width ± 0.02 mm, tab thickness ± 0.03 mm, and flatness ≤ 0.03 mm; statistical Cp/Cpk ≥ 1.33 records support ISO 9001, IATF 16949, and AS 9100 compliance.
• Post-forming stress-relief temper eliminates residual stresses, safeguarding tab ductility through repeated service interventions.
• Duplex-coated variants (zinc + epoxy powder) withstand 1 000-h xenon-arc weathering and 200 °C bake cycles without flaking or colour shift, suitable for outdoor, offshore, or mildly chemical environments.
• Every lot carries a QR-coded traceability chain linking melt chemistry, heat treatment, plating bath, and mechanical test report, providing full transparency for aerospace, medical-device, and critical-infrastructure projects.