Stainless Steel T-Nut-Four Claws Pronged Nut-Anti Corrosion Threaded Insert Description
- Leistung & Materialeigenschaften
• Premium 304/316 Stainless Steel Construction – Machined from marine-grade austenitic stainless for tensile strength ≈515 MPa, yield ≈215 MPa and elongation >40 %, with a dense chromium-oxide film that resists rust, staining and chemical attack even in coastal or high-humidity environments.
• Four-Claw Pronged Design – Four spring-tempered claws fold flush for installation, then flare outward as the mating screw engages, creating a 360° radial anchorage in wood or composite substrates. Pull-out resistance exceeds 1.2 kN in 18 mm oak or maple panels.
• Precision-Rolled Internal Threads – Available in M4–M10 and ¼-20 to ½-13 UNC, cold-rolled threads ensure smooth engagement, high fatigue life and repeated screw cycles without wear or fretting.
• Low-Profile Flanged Head – Countersunk flange sits flush with the material face for a clean appearance; optional black oxide or custom PVD finishes provide visual contrast or color coding. - Detailliertes Anwendungsspektrum
• Möbel & Cabinetry – Ideal for knock-down assemblies, drawer runners, shelf brackets and decorative panels where concealed, permanent anchorage is required.
• Carpentry & Joinery – Secures handrails, stair nosings, wardrobe frames and built-in cabinetry in residential or commercial interiors without visible fasteners.
• Stage, Set & Ausstellungsinstallationen – Bietet zuverlässige Blindseitenbefestigung in Holzbindern, Sperrholzwänden und modularen Ausstellungsständen – unterstützt dynamische Belastungen und wiederholte Montagezyklen.
• Allgemeine Holzbearbeitung & Hobbys – Perfekt für Heimwerkerprojekte, Modellbau, Sportgerätehalterungen und Instrumentenbefestigungen aus MDF, Sperrholz, Hartholz und Verbundplatten. - Mühelose Bedienung & Benutzerfreundlichkeit
• Echte blindseitige Installation – Bohren Sie das richtige Führungsloch, klopfen Sie den Einsatz bündig in Position und drehen Sie die Schraube ein. Die Krallen breiten sich hinter der Platte aus – keine Trägerplatte oder spezielle Vorrichtungen erforderlich.
• Quick, Reusable Assembly – Hammer-in seat and screwdriver or nutsetter engagement take under 5 seconds per insert. Once installed, screws can be removed and reinstalled dozens of times without compromising clamp load.
• Universal Compatibility – Works with standard wood-working bits and drivers. For high-volume jobs, compatible with pneumatic or battery-powered insertion tools for cycle times <2 s each.
• Organized Assortment Kits – Available in labeled cases containing M4–M8 and ¼-20 to ½-13 sizes (50–200 pcs), plus matching drill bits and installation guides for on-site efficiency. - Überlegene Qualität & Langfristige Zuverlässigkeit
• Internationale Standards & Zertifizierung – Hergestellt in ISO 9001-zertifizierten Anlagen zur Einhaltung der ASTM F828- und DIN-Einsteckmuttertoleranzen (±0,05 mm) und zur Gewährleistung gleichbleibender Abmessungen und Leistung.
• Strenge Tests & Rückverfolgbarkeit – Jede Charge wird einer Zug-, Scher- und Drehmoment-zu-Umdrehungs-Validierung sowie einer ≥720-stündigen neutralen Salzsprühnebelprüfung (ASTM B117) unterzogen. Vollständige Rückverfolgbarkeit der Schmelzcharge vom Rohbarren bis zum fertigen Teil mit Materialzertifikaten.
• Vibration & Ermüdungsbeständigkeit – Die Vier-Klauen-Geometrie hält die Klemmkraft unter zyklischen Belastungen, Stößen und Temperaturschwankungen aufrecht und verhindert so ein Lösen oder „Rückfallen“.
• Umweltfreundlich & Sicherheitskonformität – RoHS- und REACH-konform; frei von sechswertigem Chrom und anderen gefährlichen Stoffen. Hochreiner Edelstahl sorgt für jahrzehntelangen wartungsfreien und korrosionsbeständigen Betrieb.