Stainless Steel Phillips Modified Truss Head Self Tapping Screw for Metal-Self Drilling Screw

Artikelnummer N / A Kategorie
[Zusatz]

Menge

Stückpreis

Preis

Preisklasse: $0.015 durch $0.026

Preisklasse: $0.015 durch $0.026

Gesamt:

Preisklasse: $0.015 durch $0.026

Stainless Steel Phillips Modified Truss Head Self Tapping Screw for Metal-Self Drilling Screw Description

  1. Leistung & Materialeigenschaften
    • Dual-Grade Stainless Options: Available in AISI 304 (austenitic, tensile 500–600 MPa, excellent pitting resistance) or AISI 401 (martensitic, tensile 700–800 MPa, Rockwell hardness 30–38 HRC) to suit either superior corrosion resistance or higher wear-resistance applications.
    • Self-Drilling “TEK” Tip: Precision-ground flute hardened to RC 43–48 drills through 0.5–1.2 mm mild steel or aluminum without a pilot hole. Spiral-flute geometry rapidly evacuates chips and minimizes heat buildup to prevent galling on mating surfaces.
    • Phillips Modified Truss Head: Large Ø 9–12 mm low-profile head with a slightly domed crown and broad bearing surface distributes clamp load evenly across thin sheets, reducing pull-through on soft metals and composites.
    • Optional EPDM Washer Seal: Factory-installed elastomer washer delivers an IP65-rated barrier against moisture and dust ingress, ideal for exterior or wash-down environments.
  2. Detailliertes Anwendungsspektrum
    • Metalldach & Cladding: Secure thin-gauge aluminum or galvanized steel panels on residential and commercial roof and wall systems, soffits, fascia, and architectural façades.
    • HVAC & Ductwork Assembly: Fasten sheet-metal air ducts, plenums, flanges, and grille frames where leak-free, corrosion-resistant joints are critical.
    • Elektrische Gehäuse & Cable Management: Mount junction boxes, control panels, cable trays, and lighting fixtures in both indoor and outdoor electrical installations.
    • Leichter Rahmen & Signage: Assemble steel stud tracks, purlins, display frames, and sign brackets in commercial interiors, point-of-sale displays, and exhibition booths.
  3. Mühelose Installation & Einstellung
    • One-Step-Bohrer & Tap: Self-drilling tip eliminates separate pilot-drilling and tapping operations—cutting installation time by up to 50% and ensuring precise, repeatable hole entry even on angled or overhead surfaces.
    • Phillips Modified Drive: Deep cruciform socket resists cam-out and engages securely with standard #2 Phillips bits or low-torque screwdrivers up to 5 Nm, reducing bit-slip and operator fatigue.
    • Kontrollierte Sitzplätze & Clean Retractability: Built-in head shoulder prevents over-driving and material distortion; screws back out cleanly without enlarging the hole, facilitating rapid rework or repositioning.
  4. Überlegene Qualität & Langfristige Zuverlässigkeit
    • Standards & Certification: Produced in ISO 9001–certified facilities to ASTM A582 (304 SS) and ASTM A666 tolerances, with dimensional compliance to ANSI B18.6.4 for self-drilling screws.
    • Korrosion & Seal Integrity Testing: Passivated finish and EPDM washer assemblies endure ≥720 h neutral salt-spray per ASTM B117 with no pitting; assembled parts meet IP65 ingress protection.
    • Vollständige Rückverfolgbarkeit & Environmental Compliance: Lot-coded from melt to finished screw with material certificates, RoHS- and REACH-compliant, free of hexavalent chromium and other restricted substances—ensuring both performance and regulatory peace of mind.

Weitere Informationen

Beschichtung

Schmucklos

Durchmesser

ST3.5, ST4.2, ST4.8, ST5.5

Länge

1-1/2, 1-1/4, 1-3/4, 1'', 1/2, 100, 110, 13, 16, 19, 20, 25, 3/4, 3/8, 30, 32, 35, 38, 40, 45, 5/8, 50, 60, 63, 7/8, 70, 75, 80, 85

Hersteller

GUXIANG

Material

Edelstahl

Packungsgröße (cm)

30*20*20

Versandbedingungen

EXW Provinz Guangdong

Artikelnummer

1.000.000 Stück

Produktbezogen