  1. 性能与材料特性
    • Grade 4.8 Carbon Steel Core – Cold-forged from C35 carbon steel and heat-treated to deliver a minimum tensile strength of 400 MPa and yield strength of 240 MPa, providing reliable shear and tensile performance in light- to medium-load applications.
    • Precision Slotted Castle Profile – Machined hexagon head with six evenly spaced axial slots per ISO 4035/DIN 935 tolerances (±0.1 mm), designed to accept cotter pins or safety wires for positive mechanical locking under vibration.
    • Black Finish & Custom Color Options – Standard black-oxide conversion coating (8–12 µm) affords up to 72 h salt-spray resistance (ASTM B117) and reduced glare. Optional powder-coat or anodized finishes in any RAL color deliver enhanced corrosion protection and visual coding.
    • Compatible with Alloy-Steel Variants – Available in 42CrMo4 alloy steel upgrade for higher fatigue resistance (tensile up to 900 MPa), ideal when elevated strength or hardness (HRC 30–40) is required.
  2. 详细应用范围
    • Wheel Bearing Assemblies – Secures bearing hubs, spindle shafts and trailer axle assemblies in automotive, agricultural trailers, motorcycles and go-karts, resisting centrifugal and road-shock loads.
    • Mechanical Equipment & Machinery – Locks shafts, spindles and pulleys in gearboxes, conveyor drives, pump housings and industrial agitators across manufacturing, food processing and packaging lines.
    • Agricultural & Construction Vehicles – Used on implements, tillers, harvesters, skid-steers and backhoes where repetitive shock and dirt ingress demand positive locking and periodic maintenance.
    • DIY, Marine & Off-Road Repairs – Ideal for boat trailer wheel hubs, ATV axles and custom fabrication projects where corrosion resistance and ease of service are valued.
  3. 无劳安装和用户方便
    • Standard Wrench Compatibility – Fits common 17 mm–32 mm hex sockets and wrenches; no special tools or adapters required.
    • Quick Cotter-Pin Locking – After torquing to spec, simply align the nearest slot, insert and bend a standard split pin or safety wire—no thread-locking adhesives or jam-nuts needed.
    • Simple Repositioning & Service – Remove cotter pin, unthread nut, perform maintenance or replacement, then reinstall and re-lock; maintains slot integrity over ≥20 cycles.
    • Widely Stocked & Assortment Kits – Readily available on Amazon, eBay, Alibaba, McMaster-Carr, Fastenal, RS Components, Grainger and Würth in single sizes or mixed packs (10–200 pcs) with cotter pins and clear labeling.
  4. 优质和长期可靠性
    • ISO-Certified Manufacturing – Produced under ISO 9001 and ISO 14001 systems to DIN 6915 and ANSI/ASME B18.2.2 standards, ensuring consistent dimensions, slot geometry and material traceability.
    • Rigorous Testing Protocols – Each lot undergoes ≥72 h neutral salt-spray (ASTM B117), 5 000 installation cycles and ultrasonic crack detection to validate corrosion resistance, fatigue life and slot integrity.
    • Vibration & Shock Endurance – Mechanical lock via cotter pin prevents self-loosening under dynamic loads up to 10 g and temperature cycling from –40 °C to +120 °C.
    • Environmental & Safety Compliance – RoHS- and REACH-compliant; free of hexavalent chromium and other restricted substances, guaranteeing decades of maintenance-free, corrosion-resistant service in harsh industrial, automotive and outdoor environments.

其他信息

涂层

黑色,颜色可自定义

直径

M3、M4、M6、M8、M10、M12、M14、 M18、1/4-20、10#-24、10#-32、5/16-18、8#-32

制造商

固祥金属

材料

合金钢、碳钢

包装尺寸(厘米)

30*20*20

交货条款

EXW 广东省

SKU

1,000,000件