| Wire Diameter(mm) | 0.3, 0.4, 0.5, 0.7, 0.8, 0.9, 1.0, 1.2, 1.4, 1.5, 1.6, 1.8, 2.0, 2.5, 3.0, 4.0, 5.0 |
|---|---|
| Spring Outer Diameter(mm) | 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 2, 20, 22, 24, 25, 28, 3, 30, 32, 35, 38, 4, 40, 42, 45, 5, 50, 55, 6, 62, 7, 8, 9 |
| Spring Length(mm) | 200, 300 |
| Material | Spring steel |
| Manufacturer | GUXIANG |
| Shipping Term | EXW Guangdong Province |
| Package Size(cm) | 30*20*20 |
| SKU | 1,000,000 pieces |