description
- Superior Metal-to-Metal Sealing Performance
• Produced from ≥ 99.9 % oxygen-free copper and annealed to 45 ± 5 HV, the rings conform under bolt torque to fill micro-irregularities and create a pressure-tight, blow-out-proof seal without additional compounds.
• Fully compliant with DIN 7603 tolerances in Types A (flat), B (bevel), and C (crimped) for thread diameters M4–M60; helium-leak tests show leakage rates below 1 × 10⁻⁹ mbar · L / s at 100 bar.
• Copper’s 400 °C service limit, 385 W / m·K thermal conductivity, and low galvanic potential make the gasket ideal for high-temperature, cyclic, or conductive joints where aluminium or elastomer seals fail.
• Endurance cycling to 1 000 thermal shocks between −50 °C and +250 °C demonstrates > 95 % retention of initial tightening torque and no evidence of creep relaxation. - Broad, Cross-Industry Application Spectrum
• Fluid Power & Hydraulics: Seals banjo bolts, DIN 7421 hollow screws, and tube fittings in pumps, cylinders, and braking systems up to 400 bar.
• Engines, Turbomachinery & Compressors: Prevents oil, fuel, and coolant leakage at drain plugs, manifold unions, and sensor ports exposed to pulsating pressure and heat soak.
• Chemical Processing & Cryogenics: Provides metal-only sealing on instrumentation tappings, sampling valves, and vacuum flanges, eliminating elastomer contamination risks.
• Electronics & Renewable-Energy Equipment: Maintains EMI-shielded, gas-tight joints in liquid-cooled power converters, battery housings, and superconducting busbars. - Installer-Friendly, Time-Saving Handling
• One-piece, crush-seal design requires no preforming or adhesive—simply align the ring, tighten to the standard torque, and the copper flows to form a custom gasket in situ.
• Soft-annealed metallurgy allows minor reuse after retorque when joint surfaces remain undamaged, reducing spare-parts inventory during field service.
• Consistent wall thickness (± 0.05 mm) and deburred edges enable smooth automated feeding through vibratory bowls and pick-and-place arms on high-volume assembly lines.
• Metric size code is laser-etched on the outer rim for quick visual verification, cutting sorting time in multi-diameter kits. - Certified Quality & Long-Term Durability
• 100 % dimensional and hardness inspection with Cp/Cpk ≥ 1.67 for inner diameter, thickness, and concentricity ensures interchangeability across global standards.
• Material certificates document chemical composition to EN 1652 and residual phosphorus < 0.025 %, guaranteeing excellent brazability and low hydrogen embrittlement risk.
• Each production lot undergoes 20-cycle pressure-pulse testing from 0 to 400 bar as well as 96 h salt-spray exposure with < 5 mg/cm² mass loss, verifying corrosion resistance in harsh environments.
• Traceability is maintained via QR-coded packaging linking melt number, annealing batch, and test reports, giving engineers full transparency for aerospace, medical, and critical-infrastructure projects.