description
- Performance & Material Properties
• Countersunk Rivet Nut Design – Combines a low‐profile 120° countersunk flange with an internal hex socket drive, allowing the nut to sit flush in 5–8 mm panel holes for a smooth, snag‐free surface.
• High‐Strength Steel Construction – Machined from C1020 carbon steel and heat‐treated for ≥550 MPa tensile strength and ≥350 MPa yield strength. Precisely bored M6–M12 metric or ¼″–½″ UNC/UNF threads cold‐rolled to Class 6H/2B tolerances ensure burr‐free engagement and >10 000 insertion cycles.
• Nickel‐Plated Silver Tone Finish – Standard 10–15 µm electroless nickel plating delivers ≥240 h neutral salt‐spray resistance (ASTM B117) and a decorative silver sheen. Optional epoxy‐polyester powder‐coat in any RAL/Pantone color for enhanced corrosion resistance and décor matching.
• Compact Load Ratings – Rated for static tensile loads up to 2 000 N and shear loads up to 1 800 N per insert, ideal for securing heavy bed rails, slats and panel connectors without risk of pull‐through or deformation. - Detailed Application Range
• Furniture Bed & Headboard Assemblies – Widely used in platform beds, canopy frames, sleigh beds and upholstered headboards sold on IKEA, Wayfair, Amazon and Home Depot for hidden, high‐strength joints.
• Cribs, Bunk Beds & Nursery Furniture – Compliant with ASTM F1169 and European EN 716 safety standards; secures slatted side panels and guardrails in baby cribs and bunk‐bed systems.
• Modular Cabinets & Panel Systems – Fastens side panels, corner connectors and bracket mounts in ready‐to‐assemble wardrobes, nightstands and desks from Wayfair Commercial, Alibaba and eBay vendors.
• Specialty Seating & Storage Units – Employed in bed‐sofa hybrids, ottomans, storage benches and folding guest beds sold by Crate & Barrel, Overstock and specialist upholstery suppliers. - Effortless Operation & User Convenience
• Blind Riveting Installation – Simply insert the nut into the pre‐drilled countersink, use a standard M6–M12 rivet‐nut mandrel or hand‐tool kit to pull the blind side, and it swages into the panel—no backside access required.
• Flush, Gap‐Free Finish – The countersunk flange bonds seamlessly with wood, MDF or plywood panels, eliminating protrusions and ensuring a clean aesthetic even in visible furniture joints.
• Standard Hex Key & Driver Compatibility – Internal hex socket accepts 4 mm–8 mm Allen keys, T‐handles or power‐driver bits—no proprietary tools or special adapters needed.
• Bulk Kits & Accessory Sets – Available in assortments of 50–500 pieces with color‐coded trays, pilot‐drill guides and mandrel sets on Amazon, AliExpress, Fastenal, RS Components and Grainger for streamlined assembly lines. - Premium Quality & Long-Term Reliability
• ISO-Certified & Fully Traceable – Manufactured in ISO 9001/14001 facilities to DIN 7337 and ANSI B18.27 standards, with full batch material certification (EN 10204 3.1) available on demand.
• Rigorous Environmental & Mechanical Testing – Each lot endures ≥240 h neutral salt‐spray (ASTM B117), 1 000 installation/removal cycles, vibration testing (10–500 Hz at 5 g) and pull-through tests (>1 500 N) to ensure lasting clamp force.
• Vibration & Shock Resistance – Countersunk flange and cold‐formed blind side resist dynamic loads up to 10 g and thermal cycling from –40 °C to +80 °C, preventing loosening in transport and use.
• Environmental Compliance – RoHS-, REACH- and WEEE-compliant; free from hexavalent chromium and other restricted substances, safe for residential, commercial and children’s furniture applications.