Reamer Tek Torx/Star Head Self-Drilling Wood Sheet Metal Screw

SKU N/A Category

Quantity

Unit Price

Price

$0.06$0.07

$0.06$0.07

Total:

$0.06$0.07

描述

  1. Performance & Material Properties
    • Premium Carbon & Alloy Steel Core: Machined from quenched-and-tempered C1045 carbon steel or 4140 alloy steel, delivering tensile strengths of 800–900 MPa and Rockwell hardness of 40–48 HRC for exceptional shear and pull-out resistance when fastening heavy deck boards to steel frames.
    • Galvanized Corrosion Protection: Trivalent zinc plating (8–12 µm) with yellow or clear chromate passivation provides ≥500 hours of salt-spray resistance (ASTM B117), safeguarding fasteners against rust even in marine or road-salt environments.
    • Reamer “TEK” Self-Drilling Tip: Hardened to Rc 45–50, the flute reamer drills through 1.5–4.0 mm steel trailer rails in one pass, while its screw-point reams a clearance hole in wood decking, ensuring exact alignment without splitting or cracking.
    • Torx/Star Head & Full Thread: T30 Torx drive with deep star recess resists cam-out and accepts high-torque drivers up to 12 Nm. Full-thread shank delivers maximum clamp load and vibration resistance in wood-to-metal joints.
  2. Detailed Application Range
    • Trailer & Utility Decking: Secures pressure-treated lumber, hardwood, or composite boards to steel subframes on landscape trailers, equipment haulers, and RV slide-outs.
    • Marine & Dock Construction: Fastens marine-grade decking to galvanized or stainless steel frames for boat docks, floating platforms, and boardwalks—no pre-drilled holes needed.
    • Exterior Wood Structures: Ideal for rooftop decks, pergolas, stair treads, and outdoor stage platforms where wood meets steel support structures.
    • Industrial & Agricultural Flooring: Perfect for barn floors, mezzanine platforms, conveyor catwalks, and maintenance walkways requiring durable wood‐to‐metal connections.
  3. Effortless Installation & Operation
    • One-Step Drill, Tap & Fasten: Integrated reamer tip and self-tapping thread eliminate pre-drilling, reaming, and tapping operations—cutting installation time by up to 60 % and ensuring perfect hole alignment even on angled or overhead surfaces.
    • Torx Drive Efficiency: Deep T30 star recess provides positive bit engagement, reducing cam-out by over 50 %, minimizing operator fatigue and bit wear. Compatible with cordless, pneumatic, and hydraulic drivers.
    • Controlled Seating & Countersinking: Pan-style head with precision-machined bearing surface seats flush or slightly proud, distributing load evenly and preventing board tear-through. Anti-overdrive shoulder ensures consistent embedment depth.
    • Easy Removal & Adjustment: Screws back out cleanly without enlarging the reamed hole, enabling quick plank replacement or alignment corrections with no thread damage.
  4. Superior Quality & Long-Term Reliability
    • Certified Manufacturing & Tolerances: Produced in ISO 9001–certified facilities to ANSI B18.6.7 and DIN 7504 P standards (±0.1 mm diameter, ±0.2 mm length) for global interchangeability and dimensional accuracy.
    • Rigorous Testing & Traceability: Each batch undergoes salt-spray, drive-torque, and pull-out testing under dynamic loads. Lot-numbered from melt to finish with material certificates for full quality traceability.
    • Environmental & Safety Compliance: RoHS- and REACH-compliant, free of hexavalent chromium and other restricted substances—ensuring both worker safety and environmental stewardship.
    • Long-Term Service Life: Combined alloy-steel strength, thick galvanic barrier, and precise engineering deliver decades of maintenance-free performance, even under constant vibration, moisture, and load cycling.

其他信息

Coating

Blue Zinc, color customizable

Diameter

M3, M4, M6, M8, M10, M12, M14, M18, 1/4-20, 10#-24, 10#-32, 5/16-18, 8#-32, ST3.5, ST4.2, ST4.8, ST5.5

Length

1-1/2, 1-1/4, 1-3/4, 1'', 1/2, 100, 110, 13, 16, 19, 20, 25, 3/4, 3/8, 30, 32, 35, 38, 40, 45, 5/8, 50, 60, 63, 65, 7/8, 70, 75, 80, 85

Manufacturer

GUXIANG

Material

Alloy Steel, Carbon Steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces