描述

  1. Superior Metal-to-Metal Sealing Performance
    • Produced from ≥ 99.9 % oxygen-free copper and annealed to 45 ± 5 HV, the rings conform under bolt torque to fill micro-irregularities and create a pressure-tight, blow-out-proof seal without additional compounds.
    • Fully compliant with DIN 7603 tolerances in Types A (flat), B (bevel), and C (crimped) for thread diameters M4–M60; helium-leak tests show leakage rates below 1 × 10⁻⁹ mbar · L / s at 100 bar.
    • Copper’s 400 °C service limit, 385 W / m·K thermal conductivity, and low galvanic potential make the gasket ideal for high-temperature, cyclic, or conductive joints where aluminium or elastomer seals fail.
    • Endurance cycling to 1 000 thermal shocks between −50 °C and +250 °C demonstrates > 95 % retention of initial tightening torque and no evidence of creep relaxation.
  2. Broad, Cross-Industry Application Spectrum
    • Fluid Power & Hydraulics: Seals banjo bolts, DIN 7421 hollow screws, and tube fittings in pumps, cylinders, and braking systems up to 400 bar.
    • Engines, Turbomachinery & Compressors: Prevents oil, fuel, and coolant leakage at drain plugs, manifold unions, and sensor ports exposed to pulsating pressure and heat soak.
    • Chemical Processing & Cryogenics: Provides metal-only sealing on instrumentation tappings, sampling valves, and vacuum flanges, eliminating elastomer contamination risks.
    • Electronics & Renewable-Energy Equipment: Maintains EMI-shielded, gas-tight joints in liquid-cooled power converters, battery housings, and superconducting busbars.
  3. Installer-Friendly, Time-Saving Handling
    • One-piece, crush-seal design requires no preforming or adhesive—simply align the ring, tighten to the standard torque, and the copper flows to form a custom gasket in situ.
    • Soft-annealed metallurgy allows minor reuse after retorque when joint surfaces remain undamaged, reducing spare-parts inventory during field service.
    • Consistent wall thickness (± 0.05 mm) and deburred edges enable smooth automated feeding through vibratory bowls and pick-and-place arms on high-volume assembly lines.
    • Metric size code is laser-etched on the outer rim for quick visual verification, cutting sorting time in multi-diameter kits.
  4. Certified Quality & Long-Term Durability
    • 100 % dimensional and hardness inspection with Cp/Cpk ≥ 1.67 for inner diameter, thickness, and concentricity ensures interchangeability across global standards.
    • Material certificates document chemical composition to EN 1652 and residual phosphorus < 0.025 %, guaranteeing excellent brazability and low hydrogen embrittlement risk.
    • Each production lot undergoes 20-cycle pressure-pulse testing from 0 to 400 bar as well as 96 h salt-spray exposure with < 5 mg/cm² mass loss, verifying corrosion resistance in harsh environments.
    • Traceability is maintained via QR-coded packaging linking melt number, annealing batch, and test reports, giving engineers full transparency for aerospace, medical, and critical-infrastructure projects.

其他信息

Coating

Pickling (acid cleaning), Plain

Diameter

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

Manufacturer

GUXIANG

Material

Copper

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU