DIN137A Belleville Washer Conical Disc Spring Cup Washers 18-8 Stainless Steel

SKU N/A Category

Quantity

Unit Price

Price

$0.01

$0.01

Total:

$0.01

描述

  1. Consistent, Corrosion-Proof Spring Performance
    • Produced to DIN 137 Type A geometry from austenitic 18-8 stainless steel (≈ 304), each conical disc delivers a predictable load curve of 0.4 – 1.5 kN at 75 % deflection while remaining stable from −200 °C to +300 °C.
    • The non-magnetic, 18 % Cr / 8 % Ni alloy resists pitting, crevice attack, and atmospheric staining in marine spray, food-processing condensates, and de-icing brine—no additional plating required.
    • Cold-worked material with ≥ 950 MPa tensile strength stores high elastic energy in a compact profile, maintaining bolt preload after relaxation, gasket creep, or vibration where flat washers would loosen.
    • Chamfer-free edges and a polished contact band (Ra ≤ 1.6 µm) minimise friction scatter, giving repeatable torque-to-tension results for Class A2-70 through 10.9 fasteners.
  2. Wide Cross-Industry Application Spectrum
    • Automotive & Mobility: Controls clearance in brake caliper brackets, exhaust hangers, and drivetrain couplings exposed to heat cycles and road splash.
    • Industrial Machinery & Robotics: Compensates for bearing settle, thermal growth, and joint vibration in gearboxes, servo mounts, and packaging equipment frames.
    • Energy, HVAC & Utilities: Maintains clamp force on solar-panel clips, turbine shroud segments, and stainless pipe flanges subjected to day-night temperature swings.
    • Electronics, Medical & Food Equipment: Provides clean, non-flaking spring tension in circuit-board clamps, steriliser doors, and conveyor guides where carbon-steel parts are prohibited.
  3. Installer-Friendly, Time-Saving Handling
    • Drop-in replacement for any standard metric M3–M20 flat washer—simply position the disc with concave face toward the joint and torque to the catalogue values; no special tools or shimming needed.
    • The shallow cone and low solid height fit tight stack-ups where coil springs or locknuts cannot, enabling lighter assemblies and reduced envelope size.
    • Laser-etched diameter codes on larger sizes ensure rapid visual verification during kitting; resealable packs keep parts clean and sorted on site or in automated feeders.
    • Smooth stainless surface offers a stable, lubricant-free coefficient of friction (μ ≈ 0.15 ± 0.03), simplifying torque charts and eliminating the mess of pre-applied greases.
  4. Certified Quality & Long-Term Durability
    • 100 % dimensional inspection confirms outside diameter ±0.05 mm, thickness ±0.02 mm, cone angle ±0.5°, and parallelism ≤ 0.03 mm; Cp/Cpk ≥ 1.67 data archived under ISO 9001 and IATF 16949 systems.
    • Solution-anneal and ASTM A967 passivation remove surface iron, maximising chloride resistance; optional vibratory polishing achieves Ra ≤ 0.4 µm for hygienic or aesthetic assemblies.
    • Accelerated ageing—1 000 h salt-spray, 500 h cyclic humidity, and 2 × 10⁶ vibration pulses at 60 % deflection—shows ≥ 95 % preload retention with zero stress-corrosion cracking.
    • Each production lot carries a traceable code linking melt chemistry, hardness profile, load-deflection curve, and inspection records, giving engineers full confidence for safety-critical connections across industries.

其他信息

Coating

Plain

Diameter

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

Manufacturer

GUXIANG

Package Size(cm)

30*20*20

Material

Stainless steel

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces