描述
- High-Load, Corrosion-Protected Spring Performance
• Formed to DIN 137 Type A/B from quenched-and-tempered carbon or alloy spring steel (65 Mn, 51CrV4), the wave washer supplies a progressive load–deflection curve that preserves bolt preload despite joint relaxation, thermal expansion, or vibration.
• Typical hardness 42 – 48 HRC and three-to-six sinusoidal waves generate clamp forces from 100 N to 5 000 N while keeping the solid height ≤ 0.6 × nominal thickness, outperforming coil springs in confined spaces.
• A ≥ 8 μm electro-zinc layer with trivalent passivation delivers ≥ 120 h neutral-salt-spray resistance; optional clear, yellow, black, olive, or custom RAL/Pantone top-coats enable visual coding without altering spring rate.
• Shot-peened surfaces introduce compressive residual stress, extending fatigue life beyond 2 × 10⁶ cycles at 60 % of maximum deflection—ideal for dynamically loaded joints. - Wide-Ranging Industrial Applications
• Automotive, Rail & Off-Highway Vehicles: Maintains tension in trim panels, drivetrain covers, and exhaust brackets exposed to road shock, engine vibration, and de-icing chemicals.
• Power Transmission & Gearboxes: Compensates for thermal growth and bearing settle in housing covers, preventing seal leakage and gear noise.
• Construction, Mining & Heavy Equipment: Cushions hydraulic pump mounts, crusher housings, and boom pivots, reducing downtime caused by bolt loosening under impact loads.
• Electronics, HVAC & Renewable-Energy Systems: Provides low-profile spring compliance in inverter enclosures, fan assemblies, and solar-panel clamps subjected to daily temperature swings. - Installer-Friendly, Space-Saving Handling
• One-piece design slips under a standard screw or bolt head—no special tools or preload gauges required; simply torque to the catalogue value and the wave profile self-adjusts.
• Low stack height allows use of original fastener lengths, eliminating spacers and reducing overall assembly weight.
• Deburred edges and symmetric profile prevent galling and remove orientation errors during high-speed assembly; washers are supplied loose, on tape-and-reel, or in carrier strips to suit manual or automated lines.
• Colour-coded top-coats support quick visual size sorting, speeding workstation change-overs and minimising assembly errors. - Certified Quality & Long-Term Durability
• 100 % optical inspection verifies thickness ±0.02 mm, outer/inner diameter ±0.05 mm, wave height ±0.03 mm, and parallelism ≤ 0.05 mm; Cp/Cpk ≥ 1.67 data are archived for ISO 9001, IATF 16949, and AS 9100 traceability.
• Duplex-coated variants (zinc + epoxy) withstand 1 000 h xenon-arc weathering and 200 °C bake cycles without flaking or colour shift, ensuring dependable service in outdoor or mildly chemical environments.
• Fatigue testing confirms ≥ 95 % preload retention after 2 × 10⁶ load cycles at 50 Hz, safeguarding safety-critical joints over extended maintenance intervals.
• Lot-level QR codes link each washer to melt chemistry, heat-treat profile, coating batch, and load-deflection curve, giving engineers full confidence when specifying components for mission-critical assemblies across industries.