Retaining Washer Carbon Steel External Teeth Lock Washer -Serrated External Design-Anti Slip Vibration Resistant, Rust Resistant, Sturdy Fastener

SKU N/A Category

Quantity

Unit Price

Price

$0.01$0.02

$0.01$0.02

Total:

$0.01$0.02

description

  1. High-Grip, Corrosion-Guarded Locking Performance
    • Precision-stamped from 65 Mn spring steel and tempered to HRC 39-50 (≈ 350–500 HV), the washer’s outward-facing serrations bite simultaneously into the fastener head and joint material, producing prevailing torque that cancels vibration-induced loosening without thread damage.
    • A ≥ 8 µm electro-zinc layer sealed with trivalent passivation delivers ≥ 120 h neutral-salt-spray protection (ISO 9227); optional clear, yellow, black, olive, or custom RAL / Pantone powder top-coats push corrosion life past 1 000 h while providing instant visual coding.
    • Tooth geometry—60° flank angle and 0.25–0.45 mm height (M3–M12 range)—generates up to 30 % higher break-loose torque than flat spring washers of equal diameter, yet adds only 0.3–0.9 mm to the clamp stack.
    • Meets locking criteria of DIN 6797 Type A (external-tooth), maintaining bite after repeated tighten/loosen cycles and resisting temperatures from −50 °C to +300 °C.
  2. Cross-Industry Application Spectrum
    • Electronics & Consumer Devices: Keeps heatsink clips, PCB shields, and motor housings tight where low profile, electrical grounding through tooth contact, and colour-coded identification are valuable.
    • Automotive, Powersports & Mobility: Prevents back-off on body trim, lighting brackets, battery trays, and fairings subjected to road shock, engine vibration, and humidity.
    • Machinery, Robotics & Automation: Locks sensor mounts, guard plates, and cable glands, preserving positional accuracy during high-cycle duty, rapid axis reversals, and start-stop impacts.
    • Construction, DIY & Outdoor Equipment: Provides hidden anti-slip fastening for shelving rails, garden tools, HVAC housings, and solar-panel frames exposed to weather and mild chemicals.
  3. Installer-Friendly, Time-Saving Handling
    • Symmetric external serrations self-center under screw or nut faces, eliminating the alignment concerns of wedge-lock pairs or split pins and speeding overhead or blind installation—even with gloved hands.
    • Flat-lay geometry prevents wobble on magnetic sockets and pick-and-place nozzles, improving automated feed reliability and boosting manual throughput.
    • Supplied bulk-packed, in resealable field pouches, or on tape-and-reel strands for seamless integration with maintenance kits, bench stations, and high-speed assembly lines.
    • Optional laser-etched size code (≥ M4) enables quick visual sorting, reducing kitting errors in multi-size work cells.
  4. Proven Quality & Long-Term Durability
    • 100 % optical inspection verifies tooth height ± 0.02 mm, concentricity ≤ 0.05 mm TIR, and hardness per ISO 16228; Cp/Cpk data archived for ISO 9001 and IATF 16949 compliance.
    • Stress-relief tempering minimises hydrogen embrittlement risk and preserves high spring modulus for enduring bite through multiple service cycles.
    • Duplex-coated variants (zinc + epoxy powder) pass 1 000-h Q-SUN xenon exposure without flaking or colour shift, supporting long-term outdoor or chemical-plant use.
    • QR-coded carton labels trace every washer lot to melt chemistry, plating batch, and inspection record, ensuring full transparency for safety-critical projects in infrastructure, aerospace, and medical equipment.

Additional information

Coating

Blue Zinc, color customizable, Color Zinc

Diameter

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

Manufacturer

GUXIANG

Material

Carbon Steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces

Reviews

There are no reviews yet.

Be the first to review “Retaining Washer Carbon Steel External Teeth Lock Washer -Serrated External Design-Anti Slip Vibration Resistant, Rust Resistant, Sturdy Fastener”

Your email address will not be published. Required fields are marked *