DIN6795 French Grounding Washer

SKU N/A Category

Quantity

Unit Price

Price

$0.10$0.13

$0.10$0.13

Total:

$0.10$0.13

description

  1. High-Conductivity, Vibration-Resistant Performance
    • Manufactured to DIN 6795 from quenched-and-tempered alloy/carbon steel (typical hardness 38 – 45 HRC), the double-arched ring stores elastic energy that presses its circumferential teeth firmly into both mating surfaces. This combination supplies prevailing torque to stop back-off and forms a gas-tight electrical path for grounding or bonding.
    • A ≥ 8 µm electro-zinc layer sealed with trivalent passivation protects the base metal through 120 h neutral salt-spray (ISO 9227); optional clear, yellow, black, olive, or custom RAL/Pantone top-coats extend corrosion life past 1 000 h while offering instant circuit or size coding.
    • Tooth geometry (≈ 60 ° flank, 0.25 – 0.45 mm height in M3 – M10 sizes) delivers contact resistance below 20 mΩ after 1 000 thermal cycles (–40 °C → +120 °C) and retains ≥ 88 % of initial clamp force after transverse-vibration (Junker) testing.
    • Hydrogen-relief baking follows plating to prevent embrittlement and maintain full tensile strength for safety-critical joints.
  2. Broad, Cross-Industry Application Spectrum
    • Electrical Panels & Switchgear: Bonds door skins, hinge leaves, and bus supports, preventing electrostatic build-up or EMI leakage.
    • Renewable-Energy, EV & Rail: Grounds inverter housings, battery enclosures, and signal boxes exposed to continual vibration and outdoor weather cycles.
    • Construction Machinery & Off-Road Vehicles: Ensures reliable earth continuity across painted chassis parts, engine mounts, and sensor brackets subject to shock loading.
    • Automation, Robotics & General Manufacturing: Locks and bonds control-cabinet backplanes, cable trays, and servo-motor mounts where compact height and fast assembly are essential.
  3. Installer-Friendly, Time-Saving Handling
    • Symmetric arched profile self-centres under screw or nut faces, eliminating orientation guesswork and speeding blind, overhead, or gloved installation.
    • Spring action compensates for paint thickness, plating build-up, gasket creep, and thermal expansion, so technicians apply the same torque used with a plain washer—no recalculation or special tools.
    • Low added stack height (0.5 – 1.1 mm) means most retrofits require neither longer fasteners nor deeper counterbores.
    • Colour-coded finishes and optional laser-etched size marks (≥ M4) simplify visual sorting on mixed-size assembly lines or in maintenance kits.
  4. Verified Quality & Long-Term Durability
    • 100 % optical and mechanical inspection confirms tooth height ± 0.02 mm, arch depth ± 0.05 mm, concentricity ≤ 0.05 mm TIR, and spring rate; statistical Cp/Cpk ≥ 1.33 records support ISO 9001, IATF 16949, and AS 9100 systems.
    • Duplex-coated variants (zinc + epoxy powder) withstand 1 000-h xenon-arc weathering without flaking or colour shift, ideal for outdoor or mildly chemical environments.
    • Every production lot is QR-coded for traceability back to melt chemistry, heat treatment, plating bath, and inspection report, ensuring full supply-chain transparency.
    • Proven through cyclic vibration, temperature-swing, and salt-fog testing, these washers deliver decades of dependable grounding and anti-loosening protection across demanding industrial settings.

Additional information

Diameter

Ø4, Φ12

Manufacturer

GUXIANG

Reviews

There are no reviews yet.

Be the first to review “DIN6795 French Grounding Washer”

Your email address will not be published. Required fields are marked *