description

  1. High-Load, Corrosion-Protected Spring Performance
    • Formed to DIN 137 Type A/B from quenched-and-tempered carbon or alloy spring steel (65 Mn, 51CrV4), the wave washer supplies a progressive load–deflection curve that preserves bolt preload despite joint relaxation, thermal expansion, or vibration.
    • Typical hardness 42 – 48 HRC and three-to-six sinusoidal waves generate clamp forces from 100 N to 5 000 N while keeping the solid height ≤ 0.6 × nominal thickness, outperforming coil springs in confined spaces.
    • A ≥ 8 μm electro-zinc layer with trivalent passivation delivers ≥ 120 h neutral-salt-spray resistance; optional clear, yellow, black, olive, or custom RAL/Pantone top-coats enable visual coding without altering spring rate.
    • Shot-peened surfaces introduce compressive residual stress, extending fatigue life beyond 2 × 10⁶ cycles at 60 % of maximum deflection—ideal for dynamically loaded joints.
  2. Wide-Ranging Industrial Applications
    • Automotive, Rail & Off-Highway Vehicles: Maintains tension in trim panels, drivetrain covers, and exhaust brackets exposed to road shock, engine vibration, and de-icing chemicals.
    • Power Transmission & Gearboxes: Compensates for thermal growth and bearing settle in housing covers, preventing seal leakage and gear noise.
    • Construction, Mining & Heavy Equipment: Cushions hydraulic pump mounts, crusher housings, and boom pivots, reducing downtime caused by bolt loosening under impact loads.
    • Electronics, HVAC & Renewable-Energy Systems: Provides low-profile spring compliance in inverter enclosures, fan assemblies, and solar-panel clamps subjected to daily temperature swings.
  3. Installer-Friendly, Space-Saving Handling
    • One-piece design slips under a standard screw or bolt head—no special tools or preload gauges required; simply torque to the catalogue value and the wave profile self-adjusts.
    • Low stack height allows use of original fastener lengths, eliminating spacers and reducing overall assembly weight.
    • Deburred edges and symmetric profile prevent galling and remove orientation errors during high-speed assembly; washers are supplied loose, on tape-and-reel, or in carrier strips to suit manual or automated lines.
    • Colour-coded top-coats support quick visual size sorting, speeding workstation change-overs and minimising assembly errors.
  4. Certified Quality & Long-Term Durability
    • 100 % optical inspection verifies thickness ±0.02 mm, outer/inner diameter ±0.05 mm, wave height ±0.03 mm, and parallelism ≤ 0.05 mm; Cp/Cpk ≥ 1.67 data are archived for ISO 9001, IATF 16949, and AS 9100 traceability.
    • Duplex-coated variants (zinc + epoxy) withstand 1 000 h xenon-arc weathering and 200 °C bake cycles without flaking or colour shift, ensuring dependable service in outdoor or mildly chemical environments.
    • Fatigue testing confirms ≥ 95 % preload retention after 2 × 10⁶ load cycles at 50 Hz, safeguarding safety-critical joints over extended maintenance intervals.
    • Lot-level QR codes link each washer to melt chemistry, heat-treat profile, coating batch, and load-deflection curve, giving engineers full confidence when specifying components for mission-critical assemblies across industries.

Additional information

Coating

Black, color customizable

Diameter

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

Manufacturer

GUXIANG

Material

Alloy Steel, Carbon Steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces

Reviews

There are no reviews yet.

Be the first to review “DIN137 Carbon Steel Wave Spring Washer”

Your email address will not be published. Required fields are marked *