description

  1. Durable, High-Load Retention Performance
    • Precision-stamped from high-carbon or alloy spring steel (65 Mn / 51CrV4) and austempered to ≥ 1 000 MPa tensile strength, each external circlip clamps firmly around a shaft groove, resisting axial thrusts above 4 kN and circumferential speeds to 30 m s⁻¹ without permanent set.
    • A ≥ 8 µm electro-zinc finish with trivalent chromate passivation blocks red-rust formation for 120 h neutral-salt-spray; duplex systems (zinc + epoxy or PTFE topcoat) extend endurance past 1 000 h and can be supplied in clear, yellow, black, olive, or any RAL / Pantone hue without altering spring rate.
    • Shot-peen conditioning introduces compressive residual stress that lifts fatigue life beyond 10⁶ dynamic cycles, while radiused edges minimise stress-risers and protect mating grooves.
    • Stable from −50 °C to +200 °C, the circlip retains preload through thermal shocks and vibration, making it a compact alternative to threaded collars where axial space is limited.
  2. Wide, Cross-Industry Application Spectrum
    • Automotive & Mobility: Secures wheel-hub spacers, CV-joint components, and motorcycle sprocket carriers exposed to oil splash, grit, and road salt.
    • Industrial Machinery & Robotics: Locks gears, bearings, and pulleys on servo shafts, conveyor rollers, and packaging drives subjected to wash-downs and continuous duty.
    • Construction, Mining & Agriculture: Prevents shaft components from drifting in hydraulic cylinders, crusher rotors, and combine-harvester gearboxes operating under shock and abrasive dust.
    • Renewable Energy, HVAC & Marine: Retains turbine rotor sleeves, fan impellers, and pump couplings in coastal wind farms, chillers, and desalination plants facing chloride attack and temperature cycling.
  3. Installer-Friendly, Time-Saving Handling
    • Standard lug holes fit straight- or angled-tip snap-ring pliers; a single expand-and-release action snaps the ring fully into its groove—no screws, shims, or adhesives required.
    • Generous radial flexibility absorbs typical h8 shaft tolerances, reducing the need for precision grinding and trimming onsite.
    • Colour-coded coatings plus optional laser-etched diameter codes enable instant size identification during kitting, robotic feed, or field maintenance, cutting assembly cycle times.
    • Rings are supplied lightly oiled, nested for tangle-free removal, and packaged in resealable pouches that keep parts clean and ready for line-side use.
  4. Certified Quality & Long-Term Durability
    • 100 % optical and laser-gauge inspection verifies free diameter ± 0.03 mm, groove thickness ± 0.02 mm, flatness ≤ 0.05 mm, and lug symmetry; Cp / Cpk ≥ 1.67 data are archived under ISO 9001 and IATF 16949 quality systems.
    • Accelerated ageing—500 h cyclic humidity, 100 freeze-thaw cycles, and 2 × 10⁶ vibration pulses at 70 % proof load—shows ≥ 95 % retained radial spring force with zero coating delamination or cracking.
    • Lot-level QR codes link every ring to melt chemistry, heat-treat curve, coating batch, and dimensional record, delivering full traceability for safety-critical assemblies.
    • Compliant with RoHS and REACH, the maintenance-free zinc surface eliminates periodic lubrication, providing reliable, long-life retention across diverse industrial environments.

Additional information

Coating

Black, color customizable

Diameter

Φ1.6, Φ10, Φ12, Φ16, Φ18, Φ20, Φ22, Φ24, Φ27, Φ30, Φ32, Φ36, Φ45, Φ48, Φ50, Φ6, Φ8

Manufacturer

GUXIANG

Material

Alloy Steel, Carbon Steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces