description
- Performance & Material Properties
• Alloy Steel Construction: Bodies machined from quenched‐and‐tempered 4140 alloy steel (tensile strength up to ≈800 MPa, hardness 40–45 HRC) for maximum fatigue and shear resistance.
• Hardened Ball & Spring: High-precision bearing steel ball (≈RC 55–60) captured on a spring tempered to deliver consistent preload forces (5–30 N, depending on size).
• Protective Finish: Standard zinc-nickel plating (8–12 µm) or black-oxide coating for corrosion protection and reduced galling in industrial environments. - Detailed Application Range
• Indexing & Positioning: Provide positive “click‐stop” detents in jigs, fixtures, rotary tables, machine tool slides and assembly stations for repeatable location.
• Locking & Latching: Secure panels, doors, drawers and movable guards in automation cells, packaging machinery and medical equipment.
• Component Holding: Apply constant preload on sensors, optical mounts, circuit-board holders, and end-effector attachments in robotics and instrumentation.
• Assembly & Conveyance: Guide workpieces into precise stops on conveyors, stamping presses, textile machines and material-handling systems. - Effortless Installation & Adjustment
• Internal Hex Drive: Recessed 2 mm–8 mm Allen socket ensures slip-free engagement and controlled torque (up to 15 Nm) for rapid insertion and withdrawal.
• Self-Contained Spring Mechanism: No external spring or detent plate required—built-in spring retains the ball and provides uniform force throughout its travel.
• Quick Servicing: Standard threaded body (M3–M12) screws in and out cleanly; ball assembly can be disassembled for cleaning or replacement without special tools. - Superior Quality & Long-Term Reliability
• Precision Manufacturing: Produced in ISO 9001-certified facilities to DIN 1481/1480 tolerances (±0.1 mm on thread OD, ±0.05 mm on ball diameter) for interchangeability.
• Rigorous Testing: Each lot undergoes ball-preload measurement, dimensional inspection and corrosion testing (240 h salt-spray per ASTM B117) to ensure consistent performance.
• Full Traceability & Compliance: Material certification from melt lot to finished part; RoHS-compliant and free of magnetic anomalies—guaranteeing dependable operation in the most demanding applications.