description
- Performance & Material Properties
• 304 Stainless Steel Construction: Machined from AISI 304 (18-8) stainless steel, fully passivated to form a robust chromium-oxide barrier that resists corrosion in humid, marine, and mildly acidic environments.
• Spring-Loaded Ball-Point Tip: Hardened stainless-steel ball (≈RC 50–55) retained by a captive spring delivers a consistent preload force (5–20 N depending on size), ensuring reliable detent action without scratching or deforming mating surfaces.
• Cylindrical Slotted Head: Smooth, low-profile cylindrical head (Ø 6–12 mm) with a precision-formed slot allows greater driver engagement area and reduced cam-out compared to traditional flat-end grub screws. - Detailed Application Range
• Indexing & Detent Mechanisms: Ideal for jigs, fixtures, rotary tables, and adjustable stops in machine tools, providing a positive “click” feel for repeatable positioning.
• Latching & Position Locks: Secure doors, panels, drawers, and movable guards in automation cells, packaging machinery, and medical equipment with a smooth, snag-free head profile.
• Sensor & Instrument Mounting: Apply constant preload to optical mounts, sensors, and end-effector attachments in robotics, conveyors, and CNC systems to maintain precise alignment under vibration.
• Electronics & Control Panels: Act as board-retainers or component stoppers in electrical enclosures and test fixtures, combining corrosion resistance with a neat, low-profile head. - Effortless Operation & Adjustment
• Standard Slotted Drive: Simple flat-blade screwdriver interface accommodates a wide range of tool sizes, enabling rapid installation and field adjustments without specialty wrenches.
• Self-Contained Spring Ball: No external detent plates or additional hardware—built-in spring and ball deliver uniform force from the first use, simplifying assembly and reducing part count.
• Quick Servicing & Replacement: Slotted head and threaded body (M3–M10) screw in/out cleanly; ball-spring assembly can be disassembled for cleaning or replacement with common hand tools. - Superior Quality & Long-Term Reliability
• DIN 6325 / ISO 4026 Compliance: Manufactured to DIN 6325 tolerances (±0.1 mm on thread OD, ±0.05 mm on ball diameter) in ISO 9001–certified facilities, ensuring global interchangeability.
• Rigorous Testing: Each lot undergoes ball-preload verification, dimensional inspection, and ≥240 h salt-spray exposure per ASTM B117 to guarantee consistent detent performance and corrosion resistance.
• Full Traceability & RoHS-Compliant: Material batch and heat-treatment records maintained from melt to finished part; free of restricted substances and magnetic anomalies, delivering dependable service life in the most demanding applications.