- Precision Thickness Control & High-Strength Performance
• Produced to DIN 988 geometric tolerances in carbon and alloy spring steels (65 Mn, 51CrV4), the shims are cold-rolled and oil-tempered to 42 – 48 HRC, delivering a consistent modulus and elastic resilience in gauges from 0.05 mm to 2 mm.
• Laser-monitored slitting and flat-lapped finishing hold thickness to ±3 µm and flatness to ≤ 0.02 mm / 100 mm, enabling micron-level end-play, preload and alignment adjustments.
• Optional electro-zinc plating (≥ 8 µm) sealed with trivalent passivation provides > 120 h neutral-salt-spray protection; tinted top-coats in clear, yellow, black, olive or any RAL/Pantone code support rapid visual size sorting or functional colour coding.
• Semi-elastic metallurgy allows momentary flex without permanent set, preventing crack propagation when clamped between non-parallel faces or exposed to dynamic loads. - Broad, Cross-Industry Application Spectrum
• Power Transmission & Gearboxes: Sets precise bearing preload in helical, planetary and bevel gear stages, eliminating lash, whine and heat build-up under fluctuating torque.
• Automotive, Rail & Heavy Vehicles: Aligns differential carriers, wheel hubs and brake caliper brackets, compensating for machining tolerances and thermal expansion during life-cycle testing.
• Robotics, Machine Tools & Metrology: Calibrates spindle cartridges, linear-guide packs and ball-screw supports to maintain micron-scale positional accuracy through rapid accelerations.
• Renewable Energy, Mining & Construction: Shims generator end shields, crusher housings and hydraulic pump mounts, avoiding costly re-machining when correcting stack-up errors in the field. - Installer-Friendly, Time-Saving Handling
• Supplied loose, nested in step-gauge kits, or die-cut on peel-off sheets for clean-room or automated pick-and-place feeders; each piece is laser-etched with size and nominal thickness for instant identification.
• Flat, burr-free geometry slips between mating surfaces without adhesive or curing time—adjustments are achieved by adding or removing shims, eliminating full teardown or re-grinding.
• Ultrathin profile retains existing bolt lengths and housing depths, streamlining retrofits and service interventions; carbon-steel resilience allows slight hand-forming to follow curved seats where required.
• Colour-coded coatings and tabbed edges minimise sorting errors and speed assembly line change-overs, boosting takt-time in high-volume production. - Verified Quality & Long-Term Durability
• 100 % optical inspection confirms inner/outer diameter ±0.02 mm, concentricity ≤ 0.03 mm and burr height < 8 µm; Cp/Cpk ≥ 1.67 data are archived for ISO 9001, IATF 16949 and AS 9100 traceability.
• Fatigue tests prove ≥ 95 % preload retention after 2 × 10⁶ load cycles at 50 Hz, ensuring stability in vibrating or thermally cycling joints.
• Duplex-coated variants (zinc + epoxy powder) withstand 1 000 h xenon-arc weathering and 200 °C bake cycles without flaking or colour shift, supporting outdoor, offshore or mildly chemical environments.
• Lot-level QR codes on packaging link each shim to melt chemistry, heat-treat data, coating batch and flatness/roughness charts, delivering full transparency for safety-critical assemblies across industries.