304 Stainless Steel Torx Socket Low Head Cap Set Screw Thin Cup Head Screw

SKU N/A Category

Quantity

Unit Price

Price

$0.02$0.06

$0.02$0.06

Total:

$0.02$0.06

描述

1.High-Performance Corrosion Resistance & Strength
Machined from 304-grade stainless steel, these low-head thin socket cap screws offer a tensile strength of ≈515 MPa, yield strength of ≈205 MPa and hardness ~80 HRB. The ultra-thin head (as low as 2.5 mm for M6) and fully passivated, polished finish deliver exceptional resistance to rust, oxidation and chemical attack in compact assemblies.

2.Versatile Low-Profile Application
Engineered for flush-mount fastening where space is at a premium: consumer electronics, aerospace panels, automotive interior trim, medical instruments, precision optics and security hardware. Available in ISO metric threads M3–M12 and lengths from 4 mm to 50 mm to suit a wide range of slim‐space requirements.

3.Precision Torx Drive for Effortless Operation
Recessed Torx sockets (T10–T30) provide self-centering engagement, high torque transfer (up to 20 Nm) and virtually no cam-out. The shallow-head design minimizes protrusion and snagging, while quick insertion and removal with standard Torx bits reduce installation time and operator fatigue.

4.Certified Quality & Long-Term Reliability
Produced in ISO 9001–certified facilities to DIN 912 thin-head tolerances (±0.1 mm). Each lot undergoes dimensional inspection, torque testing and ≥240 h salt-spray resistance per ASTM B117. Full material traceability and RoHS compliance ensure consistent, long-lasting performance in demanding environments.

其他信息

Coating

Plain

Diameter

M3, M4, M6, M8, M10, M12, M14, M18, 1/4-20, 10#-24, 10#-32, 5/16-18, 8#-32

Head Type

Low Thin Cup head

Length

1-1/2, 1-1/4, 1-3/4, 1'', 1/2, 100, 110, 16, 20, 25, 3/4, 3/8, 30, 35, 40, 45, 5/8, 50, 60, 7/8, 70, 80, 85

Manufacturer

GUXIANG

Material

Stainless steel

Package Size(cm)

30*20*20

Shipping Term

EXW Guangdong Province

SKU

1,000,000 pieces