- Performance & Material Properties
• Premium 304 Stainless Steel: Machined from 18-8 (304) stainless steel with a fully passivated, polished finish for superior corrosion resistance.
• Mechanical Strength: Tensile strength ≈515 MPa, yield strength ≈205 MPa and hardness ~80 HRB, delivering reliable clamp force in dynamic and static loads.
• Flat-Point Tip Design: Precision-ground flat end distributes pressure evenly across mating surfaces, minimizing shaft marring and ensuring consistent holding power. - Detailed Application Range
• Shaft and Collar Locking: Ideal for securing collars, gears, pulleys and couplings on motor and gearbox shafts without deep indentations.
• Instrumentation & Electronics: Fastens circuit-board standoffs, sensor mounts and optical components where low profile and precise positioning are critical.
• Robotics & Automation: Locks linear guide blocks, end-effector fixtures and rotary joints in robotic arms and pick-and-place machines.
• Food, Marine & Medical Equipment: Corrosion-resistant construction suits wash-down environments, marine hardware and non-magnetic medical assemblies. - Effortless Installation & Adjustment
• Internal Hex Drive: Recessed Allen socket (sizes 1.5 mm–8 mm) ensures slip-free engagement, accurate torque application (1–10 Nm) and minimal cam-out.
• Self-Seating Flat Point: Cuts its own mating surface for a self-sealing fit; no washers or adhesives required, simplifying parts count and assembly steps.
• Repositionable & Removable: Flat-point tip allows multiple adjustments without damaging substrates, reducing downtime during service or calibration. - Certified Quality & Long-Term Reliability
• Tight Tolerances & Standards: Produced in ISO 9001–certified facilities to DIN 916 tolerances (±0.1 mm), guaranteeing interchangeability and precise fit.
• Rigorous Testing: Each batch undergoes dimensional inspection, drive-torque consistency testing and ≥240 h salt-spray exposure per ASTM B117.
• Full Traceability & Compliance: Material lot tracking from melt to finished part, RoHS-compliant and free of magnetic anomalies—ensuring consistent performance in the most demanding environments.